Bactericidal environment-friendly coating
An environmentally friendly paint and fungicide technology, applied in the field of paint processing, can solve problems such as human health and environmental hazards, and achieve the effects of low cost, easy source of raw materials, and simple ingredients
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Embodiment one: a kind of preparation method of the environment-friendly paint of sterilization, is made up of the composition of following weight component: 42 parts of natural diatomites, 32 parts of modified nano-clay minerals, 4 parts of curing agents, 10 parts of bactericides, thickening 0.4 parts of agent, 125 parts of deionized water.
[0027] The processing method of described coating comprises the following steps,
[0028] S1, get each raw material by weight component;
[0029] S2. Grinding diatomite and modified nano-clay minerals, and sieving through a 50-mesh screen after grinding, to obtain powdered diatomite and powder-modified nano-clay minerals;
[0030] S3. Put the powdered diatomite and powder modified nano-clay minerals prepared in step S2 into a blender, and add a bactericide, and stir, the speed of the blender is 240r / min, and the stirring time is 50min, and the stirring material 1 is obtained;
[0031] S4. Add the curing agent, thickener and deio...
Embodiment 2
[0033] Embodiment two: a kind of preparation method of the environment-friendly paint of sterilization, is made up of the composition of following weight component: 48 parts of natural diatomites, 38 parts of modified nano-clay minerals, 6 parts of curing agents, 11 parts of bactericides, thickeners 0.5 parts of agent, 135 parts of deionized water.
[0034] The processing method of described coating comprises the following steps,
[0035] S1, get each raw material by weight component;
[0036] S2. Grinding diatomite and modified nano-clay minerals, and sieving through a 60-mesh screen after grinding, to obtain powdered diatomite and powder-modified nano-clay minerals;
[0037] S3. Put the powdered diatomite and powder modified nano-clay minerals prepared in step S2 into a blender, add a bactericide, and stir, the speed of the blender is 280r / min, and the stirring time is 55min, to obtain a blender 1;
[0038] S4. Add the curing agent, thickener and deionized water into the s...
Embodiment 3
[0040] Embodiment three: a kind of preparation method of the environment-friendly paint of sterilization, is made up of the composition of following weight component: 32 parts of natural diatomites, 24 parts of modified nano-clay minerals, 3 parts of curing agents, 9 parts of bactericides, thickening 0.3 parts of agent, 105 parts of deionized water.
[0041] The processing method of described coating comprises the following steps,
[0042] S1, get each raw material by weight component;
[0043] S2. Grinding diatomite and modified nano-clay minerals, and sieving through a 40-mesh sieve after grinding, to obtain powdered diatomite and powder-modified nano-clay minerals;
[0044] S3. Put the powdered diatomite and powder modified nano-clay minerals prepared in step S2 into a blender, add a bactericide, and stir, the speed of the blender is 220r / min, and the stirring time is 40min, and the stirring material 1 is obtained;
[0045] S4. Add the curing agent, thickener and deionize...