Method for preparing wet-mixed mortar by utilizing waste residue nickel slag
A technology of mortar and nickel slag, which is applied to the new technology products of building materials or the field of high efficiency, energy saving and environmental protection, can solve the problems of less than 2% utilization rate, ecological environment pollution, difficult development and utilization, etc., and achieve low production cost, less production raw materials, The effect of strong bond strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The invention discloses a method for preparing wet-mixed mortar by using waste nickel slag. The waste nickel slag with a water content of 25% discharged from a nickel product enterprise is mechanically passed through a 20-mesh sieve, and the weight percentage is 100% and 325 general purpose. The cement is calculated as 5% by weight, and they are evenly stirred by a mixing mixer to obtain wet-mixed mortar.
[0019] In the present invention, the amount of wet-mixed mortar prepared by using waste nickel slag instead of natural sand is 100%, and the prepared wet-mixed mortar can be applied to plastering mortar, ground mortar, internal and external wall mortar, special mortar, ceramic tile in construction engineering construction Mortar, waterproof mortar.
[0020] After measurement, the technical indicators of the prepared wet-mixed mortar products are setting time 230 minutes; water retention rate 101%; 28-day shrinkage rate 0.05%; The 28-day compressive strength is 7.9mp...
Embodiment 2
[0022] The invention discloses a method for preparing wet-mixed mortar by using waste nickel slag. The waste nickel slag with a water content of 25% discharged from a nickel product enterprise is mechanically passed through a 20-mesh sieve, and the weight percentage is 100% and 325 general purpose. The cement is calculated as 10% by weight, and it is evenly stirred by a mixing mixer to obtain a wet-mixed mortar.
[0023] In the present invention, the amount of wet-mixed mortar prepared by using waste nickel slag instead of natural sand is 100%, and the prepared wet-mixed mortar can be applied to plastering mortar, ground mortar, internal and external wall mortar, special mortar, ceramic tile in construction engineering construction Mortar, waterproof mortar.
[0024] After measurement, the technical indicators of the wet-mixed mortar prepared by the present invention are setting time 245 minutes; water retention rate 105%; 28-day shrinkage rate 0.06%; The 28-day compressive s...
Embodiment 3
[0026] The invention discloses a method for preparing wet-mixed mortar by using waste nickel slag. The waste nickel slag with a water content of 25% discharged from a nickel product enterprise is mechanically passed through a 20-mesh sieve, and the weight percentage is 100% and 325 general purpose. The cement is calculated as 15% by weight, and it is evenly stirred by a mixing mixer to obtain a wet-mixed mortar.
[0027] In the present invention, the amount of wet-mixed mortar prepared by using waste nickel slag instead of natural sand is 100%, and the prepared wet-mixed mortar can be applied to plastering mortar, ground mortar, internal and external wall mortar, special mortar, ceramic tile in construction engineering construction Mortar, waterproof mortar.
[0028] After measurement, the technical indicators of the wet-mixed mortar prepared by the present invention are setting time 235 minutes; water retention rate 103%; The daily compressive strength is 25.5mpa and 53.9mpa...
PUM
| Property | Measurement | Unit |
|---|---|---|
| flexural strength | aaaaa | aaaaa |
| compressive strength | aaaaa | aaaaa |