Water-based paint spraying process

A technology of water-based paint and water-based primer, which is applied in coatings, devices for coating liquid on the surface, and surface pretreatment, etc., can solve the problems of low adhesion of water-based paint, great harm to human body, and delamination of water-based paint. Achieve the effect of improving environmental protection performance, avoiding the release of benzene and VOC, and ensuring quality

Inactive Publication Date: 2020-08-28
安徽志邦全屋定制有限公司
View PDF7 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The water-based paint coating process is a new type of wood veneer water-based paint application technology, which is mainly used in furniture, doors, windows, wall panels, etc. The mixed oil products on the market generally include PU bottom PU surface, NC bottom NC surface and PU bottom water-based surface. , the use of oily polyester paint is mostly oily polyester paint, its environmental protection performance, safety performance, benzene and VOC release are very high in the later stage, which not only pollutes the environment, but also is extremely unsafe; and in the use process of these water-based paints, because water-based paints cannot Directly acting on veneer and logs, it is necessary to use ethanol-based water-based paint for wood primary isolation, and water-based paint must be diluted with ethanol-containing water-based paint, so the operation is extremely harmful to the human body, and the ethanol volatilizes in the later stage to produce color separation. Ethanol volatilizes, resulting in flaky or speckled color, especially dark color is the most serious, turning yellow and mottled
In addition, due to the low adhesion of water-based paint, there will be delamination of water-based paint

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0032] Step 1. Spray the water-based color by artificial oil pump spraying method. The coating amount is 120g / ㎡. After coating, wipe it manually and dry it after wiping. In this embodiment, the water-based color includes solvent and pigment, and the solvent includes base material and Water, the base material includes water-based acrylic acid, water-based base material, and water-based activator, and the solvent includes: 30% of water-based acrylic acid, 20% of water-based base material, 20% of water-based activator, and 30% of pure water, and the present embodiment uses LCFACR-25 water-based acrylic, VEA255-25 water-based base material, D1072-20 water-based activator produced by Italy ICA Group, the pigments use INK series color essence and CNA series color paste, the mass percentage of pigment and base material is 2:100. Mix the base material, purified water and pigments before spraying, wipe directly after spraying, and dry after wiping. The drying temperature is above 30°C a...

Embodiment 2

[0041] Step 1. Apply water-based color by machine roller coating, and the coating amount is 130g / ㎡. In this embodiment, the water-based color includes solvent and pigment, the solvent includes base material and water, the base material includes water-based acrylic, water-based Material, water-based activator, and solvent include: 30% water-based acrylic acid, 15% water-based base material, 15% water-based activator, 40% purified water, and the present embodiment uses LCFACR-25 water-based acrylic acid produced by Italy ICA Group , VEA255-25 water-based base material, D1072-20 water-based activator, the pigment uses INK series color essence, and the mass percentage of pigment and base material is 4:100. Mix the base material, purified water and pigments before spraying, wipe directly after spraying, and dry after wiping. The drying temperature is below 30°C and the drying time is 6 hours.

[0042] Step 2. Spray the product after the color spraying and drying in step 1 with a wa...

Embodiment 3

[0050] Step 1. Spray the water-based color by artificial oil pump spraying method, and the coating amount is 150g / ㎡. In this embodiment, the water-based color includes solvent and pigment, the solvent includes base material and water, the base material includes water-based acrylic acid, water-based base material , water-based activator, the solvent includes by mass percentage: 30% water-based acrylic acid, 10% water-based base material, 10% water-based activator, 50% purified water, while the present embodiment uses LCFACR-25 water-based acrylic acid produced by Italy ICA Group, VEA255-25 water-based base material, D1072-20 water-based activator, the pigment adopts CNA series color paste, and the mass percentage of pigment and base material is 6:100. Mix the base material, purified water and pigments before spraying, wipe directly after spraying, and dry after wiping. The drying temperature is above 30°C and the drying time is 4 hours.

[0051] Step 2. Spray the product after ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
Login to view more

Abstract

The invention discloses a water-based paint spraying process which comprises the following steps: performing water-based color coating for the first time with the coating weight of 120-150g / m<2>, drying after coating, performing water-based color fixing primer coating with the coating weight of 110-120g / m<2> after drying, drying after coating, and performing water-based color fixing primer sandingafter drying; carrying out water-based primer coating with the coating weight of 140-150g / m<2> after sanding, and performing drying sanding after coating; and after sanding, performing water-based finish paint spraying with the coating weight of 130-160 g / m<2>. The water-based pigment is prepared from water-based acrylic acid, a water-based base material, a water-based activating agent, purifiedwater and color; in addition, the water-based pigment can be directly coated on wood veneer or logs; and aqueous sealing primer is not needed, so that a production process is simplified, production cost is reduced, production efficiency is improved, the water-based color is directly roller coated or sprayed on the wood veneer or the log, the phenomena of color separation and yellowing caused by ethanol volatilization are effectively avoided, and the product quality is improved.

Description

technical field [0001] The invention relates to the technical field of water-based paint spraying, in particular to a water-based paint spraying process. Background technique [0002] Any coating that uses water as a solvent or as a dispersion medium can be called a water-based paint. Water-based paint includes three types: water-soluble, water-diluted, and water-dispersed (latex paint). [0003] The water-based paint coating process is a new type of wood veneer water-based paint application technology, which is mainly used in furniture, doors, windows, wall panels, etc. The mixed oil products on the market generally include PU bottom PU surface, NC bottom NC surface and PU bottom water-based surface. , the use of oily polyester paint is mostly oily polyester paint, its environmental protection performance, safety performance, benzene and VOC release are very high in the later stage, which not only pollutes the environment, but also is extremely unsafe; and in the use proce...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): B05D7/08B05D3/12C09D133/04
CPCB05D7/08B05D3/12B05D7/584C09D133/04B05D2502/00
Inventor 储逵张文斌
Owner 安徽志邦全屋定制有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products