[0038] The preparation method of antistatic textile includes the following steps:
[0039] (1) 7 parts by weight of white latex, 6 parts by weight of ethanol, 3 parts by weight of titanium dioxide, 4 parts by weight of trihydroxyethyl methyl quaternary ammonium methyl sulfate, 2 parts by weight of tridecafluorooctyl trimethoxysilane, 80 parts by weight Parts by weight of water, stirring at a speed of 300r / min for 20min and mixing evenly to obtain an antistatic finishing agent for fabric
[0040] (2) Immerse the fabric in the fabric antistatic finishing agent at 40°C for 20 minutes, and the mass ratio of the fabric to the fabric antistatic finishing agent is 1:10; then the immersed fabric is subjected to liquefaction to control the surplus rate of 75wt%. Drying at 80°C for 5 hours, the antistatic textile is obtained.
Embodiment 2
[0042] The preparation method of antistatic textile includes the following steps:
[0043] (1) Combine 7 parts by weight of white latex, 6 parts by weight of ethanol, 3 parts by weight of titanium dioxide, 2 parts by weight of tridecafluorooctyltrimethoxysilane, 4 parts by weight of stearamide ethyldiethylbenzylammonium chloride, 80 parts by weight of water, stirring at a speed of 300r / min for 20min and mixing uniformly to obtain an antistatic finishing agent for fabric
[0044] (2) Immerse the fabric in the fabric antistatic finishing agent at 40°C for 20 minutes, and the mass ratio of the fabric to the fabric antistatic finishing agent is 1:10; then the immersed fabric is subjected to liquefaction to control the surplus rate of 75wt%. Drying at 80°C for 5 hours, the antistatic textile is obtained.
Embodiment 3
[0046] The preparation method of antistatic textile includes the following steps:
[0047] (1) Combine 7 parts by weight of white latex, 6 parts by weight of ethanol, 3 parts by weight of titanium dioxide, 3 parts by weight of trihydroxyethyl methyl quaternary ammonium methyl sulfate, 2 parts by weight of tridecafluorooctyl trimethoxysilane, 1 Parts by weight of stearyl amide ethyl diethyl benzyl ammonium chloride, 80 parts by weight of water, stirring at 300 r / min for 20 minutes and mixing uniformly to obtain an antistatic finishing agent for fabrics;
[0048] (2) Immerse the fabric in the fabric antistatic finishing agent at 40°C for 20 minutes, and the mass ratio of the fabric to the fabric antistatic finishing agent is 1:10; then the immersed fabric is subjected to liquefaction to control the surplus rate of 75wt%. Drying at 80°C for 5 hours, the antistatic textile is obtained.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More