Embodiment 2
[0026] The invention provides a technical scheme of a coating additive and a preparation method thereof: a coating additive and a preparation method thereof, and the preparation method of the coating additive specifically has the following steps:
[0027] The first step: select 12 parts of linoleic acid soap, 5 parts of rosin acid soap, 5 parts of toughening agent, 2 parts of activated calcium carbonate particles, 15 parts of polymerized vegetable oil, 1 part of white carbon black, 1 part of metal soap, methyl 15 parts of silicone oil, 5 parts of fluorine-containing surfactant, 15 parts of polyacrylate, 2 parts of nano-titanium oxide, 1 part of ultraviolet absorber and 100 parts of distilled water;
[0028] The second step: Immediately after adding 100 parts of distilled water into the high-speed disperser, sequentially add linoleic acid soap, rosin acid soap, activated calcium carbonate particles, polymerized vegetable oil, white carbon black, metal soap, methyl silicone oil, ...
Embodiment 3
[0034] The invention provides a technical scheme of a coating additive and a preparation method thereof: a coating additive and a preparation method thereof, and the preparation method of the coating additive specifically has the following steps:
[0035] The first step: select 15 parts of linoleic acid soap, 5 parts of rosin acid soap, 5 parts of toughening agent, 5 parts of activated calcium carbonate particles, 20 parts of polymerized vegetable oil, 1 part of white carbon black, 1 part of metal soap, methyl 15 parts of silicone oil, 3 parts of fluorine-containing surfactant, 15 parts of polyacrylate, 2 parts of nano-titanium oxide, 2 parts of ultraviolet absorber and 150 parts of distilled water;
[0036] The second step: Immediately after adding 150 parts of distilled water into the high-speed disperser, sequentially add linoleic acid soap, rosin acid soap, activated calcium carbonate particles, polymerized vegetable oil, white carbon black, metal soap, methyl silicone oil,...
Embodiment 4
[0042] The invention provides a technical scheme of a coating additive and a preparation method thereof: a coating additive and a preparation method thereof, and the preparation method of the coating additive specifically has the following steps:
[0043] The first step: select 15 parts of linoleic acid soap, 5 parts of rosin acid soap, 5 parts of toughening agent, 5 parts of activated calcium carbonate particles, 20 parts of polymerized vegetable oil, 2 parts of white carbon black, 2 parts of metal soap, methyl 20 parts of silicone oil, 3 parts of fluorine-containing surfactant, 15 parts of polyacrylate, 10 parts of nano-titanium oxide, 1 part of ultraviolet absorber and 100 parts of distilled water;
[0044] The second step: Immediately after adding 100 parts of distilled water into the high-speed disperser, sequentially add linoleic acid soap, rosin acid soap, activated calcium carbonate particles, polymerized vegetable oil, white carbon black, metal soap, methyl silicone oi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com