[0037] refer to figure 1 , the invention discloses a method for preparing a solar panel for electric curtains, which comprises the following steps:
[0038] S1: provide the substrate;
[0039] Specifically, the substrate can be glass, ceramic plate, stainless steel, but not limited thereto. Preferably, in the invention, the substrate is made of ITO transparent conductive glass, which has excellent compatibility with the silicon structure and excellent conductivity.
[0040] S2: Texturing the front side of the substrate;
[0041] Specifically, S2 includes:
[0042] S21: forming an ink protection layer on the back side of the substrate;
[0043] Specifically, a screen printing process can be used to print a layer of acid-resistant ink on the back of the substrate to obtain an ink protective layer;
[0044] S22: putting the substrate provided with the ink protection layer into a mixed solution of hydrogen peroxide and concentrated sulfuric acid, and corroding at 60-80° C. fo...
Embodiment 1
[0076] This embodiment provides a method for preparing a solar panel for electric curtains, which includes:
[0077] (1) Provide the substrate;
[0078] Among them, the substrate is ITO transparent conductive glass;
[0079] (2) Texturing the front side of the substrate;
[0080] Specifically, an ink protective layer is first formed on the back of the substrate, then put into a mixed solution of hydrogen peroxide and concentrated sulfuric acid with a volume ratio of 1:3, and corroded for 6 hours; after taking it out, wash off the ink protective layer with NaOH.
[0081] (3) cleaning the textured substrate with a first solution containing an aminosilane coupling agent;
[0082] Specifically, the substrate is ultrasonically cleaned with pure water for 1 hour, and then soaked in ethanol for 1 hour; then the substrate is put into 1 vol% γ-aminopropyltrimethoxysilane aqueous solution and soaked for 6 hours.
[0083] (4) sequentially forming an n-type amorphous silicon layer, an ...
Embodiment 2
[0093] This embodiment provides a method for preparing a solar panel for electric curtains, which includes:
[0094] (1) Provide the substrate;
[0095] Among them, the substrate is ITO transparent conductive glass;
[0096] (2) Texturing the front side of the substrate;
[0097] Specifically, an ink protective layer is first formed on the back of the substrate, then put into a mixed solution of hydrogen peroxide and concentrated sulfuric acid with a volume ratio of 1:2, and corroded for 8 hours; after taking it out, use NaOH to wash off the ink protective layer.
[0098] (3) cleaning the textured substrate with a first solution containing an aminosilane coupling agent;
[0099] Specifically, first use pure water to ultrasonically clean for 50 minutes, and then soak in ethanol for 1 hour; 5h.
[0100] (4) sequentially forming an n-type amorphous silicon layer, an i-type amorphous silicon layer and a p-type amorphous silicon layer on the front side of the cleaned substrate;...