A technology for decorative panels and panels, applied in building materials, structural elements, building components, etc., can solve the problems of high price, high cost and heavy weight of aluminum-plastic panels, and achieve the effects of convenient construction, good weather resistance and light weight.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] First dissolve 25 kg of magnesium chloride in 15 kg of water, then 45 kg of magnesium oxide, perlite
[0024] Add 15 kg into it and mix evenly; add the above ingredients into the discharge port of the paving machine; place the flat formwork on the paving machine, clamp the 3 layers of glass fiber mesh cloth, and carry out rolling coating; after forming, cure at room temperature for 8 hours ; After demoulding, immerse in water for 10 hours for desalination; dry and then shape; that is, the finished flat decorative board.
Embodiment 2
[0026] First dissolve 35 kg of magnesium chloride in 20 kg of water, then add 20 kg of magnesium oxide and 25 kg of perlite and mix evenly; add the above ingredients to the discharge port of the paving machine; put the flat template on the paving machine, put 10 Layers of glass fiber mesh are clamped and rolled for coating; after molding, it is cured at room temperature for 8 hours; after demolding, it is soaked in water for 10 hours for desalination; after drying, it is shaped; that is, the finished flat sound insulation board with good thermal insulation, sound insulation and fire prevention effects.
Embodiment 3
[0028] Dissolve 40 kg of magnesium chloride in 30 kg of water, then 15 kg of magnesium oxide, 5 kg of perlite, 5 kg of titanium dioxide, and 5 kg of gypsum powder. Add it and mix evenly; add the above ingredients into the discharge port of the paving machine; place the profiled formwork of the corner liner on the paving machine, clamp the 3 layers of glass fiber mesh cloth, and carry out rolling coating; after forming, cure at room temperature for 8 Hours; after demoulding, immerse in water for 10 hours for desalination; after drying, shaping; it is the finished corner board.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com