Needle of colored beading and preparation method
A technology for colored glass and a manufacturing method, applied in printing, office supplies, pushpins, etc., can solve the problems of environmental pollution, complex manufacturing process, easy falling off, etc., and achieve the effect of pollution-free production process, simple manufacturing process and good finish.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0009] The first step is to prepare a needle strip of medium carbon steel material with a diameter of 0.65mm and a colored glass rod with a diameter of 6mm. The front end of the needle strip has a needle point, and the rear end of the needle strip is flattened. The material of the colored glass rod can be soda-lime glass, and the parts by weight of its composition are: 10 parts of SiO 2 , 1.2 parts of feldspar powder, 4 parts of Na 2 CO 3 , 2 parts of Na 2 B 4 o 7 And an appropriate amount of chromium oxide colorant (green);
[0010] The second step is to manually place one end of the colored glass rod on the burner of an oxygen and acetylene gas mixed burner for heating. When the temperature of the end of the colored glass rod reaches about 600°C, it begins to melt. The end of the glass rod is bonded together, and the amount of glass bonded to the rear end of the needle bar is gradually increased by manually rotating the needle bar to form a ball head. When the diameter...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More