Protein functional fiber
A functional fiber and protein technology, applied in the field of synthetic fibers, can solve the problems of no functional effect of fibers, skin-friendly properties of synthetic fibers, poor air permeability, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] Embodiment 1, get animal protein and polyvinyl alcohol to make spinning stock solution, the dry solid content A that contains animal protein in this spinning stock solution is 50 weight parts, the dry solid content B of polyvinyl alcohol is 49.5 weight parts, spinning After the silk stock solution is degassed, wet spinning is adopted, and the synthetic fiber tow coming out of the spinning machine enters the coagulation bath containing alumina. The dry solid content C of alumina is 0.5 parts by weight, and then the tow is passed through the air After drafting, wet bath drafting, dry drafting and heat setting, semi-finished products are made, and semi-finished products are finished after finishing and acetalization.
Embodiment 2
[0047] Embodiment 2, get vegetable protein and polyvinyl alcohol to make spinning stock solution, the dry solid content A that contains vegetable protein in this spinning stock solution is 67 weight parts, the dry solid content B of polyvinyl alcohol is 10 weight part, spinning After the silk stock solution is degassed, wet spinning is adopted. The synthetic fiber tow coming out of the spinning machine enters the coagulation bath containing 13 parts by weight of ferric oxide, and then the tow is drawn by air, wet bath and Dry drafting, and then into a sizing solution containing 10 parts by weight of ferroferric oxide to make a semi-finished product, which becomes a finished product after finishing and acetalization.
Embodiment 3
[0048] Embodiment 3, get vegetable protein and polyacrylonitrile and make spinning stock solution, the dry solid content A that contains vegetable protein in this spinning stock solution is 27.2 weight parts, the dry solid content B of polyacrylonitrile is 55 weight parts, spinning The silk stock solution is degassed and wet-spun, and the synthetic fiber tow coming out of the spinning machine enters the coagulation bath containing 9.8 parts by weight of ferric oxide, and then the tow is drawn by air and wet bath , dry drawing and heat setting to make a semi-finished product, and then enter the dyeing and finishing bath containing 8 parts by weight of silicon dioxide to dye and finish the semi-finished product to become a finished product.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com