Passiveness sampling method
A passive sampler, hollow technology, applied in sampling devices, instruments, measuring devices, etc., to achieve the effect of low cost, low production cost, and reduced sample volume
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Such as figure 1 As shown, adopt the method provided by the invention to collect bisphenol A in environmental water sample 1, concrete steps are as follows:
[0028] (1) Fill the inner cavity of the cut 5mm length polypropylene hollow fiber membrane section with water;
[0029] (2) Soak the polypropylene hollow fiber membrane section filled with water in the inner cavity for 5 seconds in n-octanol, so that the micropores on the membrane wall of the polypropylene hollow fiber membrane section are filled with n-octanol to form a hollow fiber support Liquid film passive sampler 2;
[0030] (3) The hollow fiber-supported liquid membrane passive sampler 2 is taken out from n-octanol, and placed in water for cleaning to remove excess n-octanol adsorbed on its surface;
[0031] (4) Submerge the cleaned hollow fiber supported liquid membrane passive sampler 2 in the sample solution 1 to be sampled for 20 minutes to complete the sampling;
[0032] (5) Take out the passive sam...
Embodiment 2
[0036] In this embodiment, the hydrophobic hollow fiber membrane is selected from a 5 mm polyvinylidene fluoride hollow fiber membrane section, the water-insoluble organic solvent is selected from n-undecane, and the polyvinylidene fluoride hollow fiber membrane section filled with water in the inner cavity Soak in n-undecane for 60 seconds, the target substance is nonylphenol in the environmental water sample, the hollow fiber supported liquid membrane passive sampler is immersed in the environmental water sample for 1 day, and the target substance can be sampled from The solvent that dissolves out in the device selects normal hexane, and others are identical with embodiment 1.
Embodiment 3
[0038] In this embodiment, the hydrophobic hollow fiber membrane is selected from a 5mm polytetrafluoroethylene hollow fiber membrane section, the water-insoluble organic solvent is selected from n-hexyl ether, and the polytetrafluoroethylene hollow fiber membrane section filled with water in the inner cavity is Soak in n-hexyl ether for 30 seconds, the target substance is nonylphenol in the environmental water sample, the hollow fiber supported liquid membrane passive sampler is immersed in the environmental water sample for 2 days, the other is the same as in Example 1.