A carbomer eye and gel technology, which is applied in the field of medicine, can solve the problems of large loss of eye drops, short residence time, and restrictions on the curative effect of carbomer eye drops, etc., so as to prolong the residence time, improve the curative effect, enrich the The effect of the drug dosage form
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Prescription: Carbomer 940 10g Hydrochloric acid (0.05mol / L) 400ml Sodium citrate 9.6g
[0030] Methylcellulose 5.0g Phenylethyl alcohol 0.5g Ethanol 5ml
[0031] Sodium Chloride 1.0g PEG-1000 20g
[0032] PEG-400 5g water for injection appropriate amount
[0033] Preparation method: Heat water for injection to boil, cool to 80°C, add Carbomer 940, dissolve phenylethyl alcohol in ethanol, add dropwise to the above solution while stirring, add sodium citrate, stir for more than 30 minutes, then add hydrochloric acid After stirring, filter through a microporous membrane (0.22μm), heat the filtrate to 40°C, add sodium chloride, methylcellulose, PEG-1000 and PEG-400 while hot, and stir to room temperature (18-25°C ), add water for injection to make up the weight to 1000 milliliters, stir to make it form a uniform gel, and aseptically pack it.
Embodiment 2
[0035] Prescription: Carbomer 940 10g Sulfuric acid (0.05mol / L) 200ml
[0036] Sodium Citrate 8.8g Methylcellulose 5.0g Benzyl Alcohol 0.5g
[0037] Ethanol 5ml Sodium Chloride 2.0g PEG-1000 70g
[0038] Appropriate amount of water for injection
[0039] Preparation method: heat water for injection to boil, cool to 80°C, add carbomer 940, dissolve benzyl alcohol in ethanol, add dropwise to the above solution while stirring, add sodium citrate, stir for more than 30 minutes, then add sulfuric acid After stirring, filter through a microporous membrane (0.22μm), heat the filtrate to 40°C, add sodium chloride, methylcellulose and PEG-1000 while hot, stir to room temperature (18-25°C), and add Make up the weight with water for injection to 1000 ml, stir to make it form a uniform gel, and aseptically pack it.
Embodiment 3
[0041] Prescription: Carbomer 940 10g Sodium Hydroxide (0.1mol / L) 200ml
[0042] Boric acid 5.6g Methylcellulose 5.0g Sodium benzoate 0.5g
[0043] Ethanol 5ml Sodium Chloride 5.0g PEG-4000 100g
[0044] Appropriate amount of water for injection
[0045] Preparation method: heat water for injection to boil, cool to 80°C, add Carbomer 940, add sodium citrate, sodium hydroxide and sodium benzoate, stir for more than 30 minutes, then add boric acid and stir, pass through a microporous membrane (0.22 μm), the filtrate was heated to 40°C, PEG-4000 and methylcellulose were added while it was hot, stirred to room temperature (18-25°C), and water for injection was added to make up the weight to 1000 ml, and stirred to form a uniform Gel, aseptically dispensed.