High temperature resistant surface-insulated FeCrAl electrothermal alloy and preparation method thereof
An electric heating alloy, high temperature resistant technology, applied in the direction of heating element materials, metal material coating process, solid state chemical plating, etc., can solve the problems of small temperature coefficient of resistance, low price, uneven heating temperature of electric heating wire, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Embodiment 1, high temperature resistant surface insulating FeCrAl electrothermal alloy, characterized in that: the FeCrAl electrothermal alloy substrate is provided with a high temperature resistant insulating composite alumina protective layer containing rare earth.
[0015] The preparation method provided by the present invention is as follows: first, the FeCrAl electrothermal alloy product is degreased and derusted, and then rinsed; secondly, the rinsed product is immersed in a sol-gel containing rare earth, and it is taken out and dried after about 10 minutes. ; Finally, between 850-950 ° C in a protective atmosphere for about 180 minutes of heat treatment to obtain a FeCrAl electric heating alloy product with high temperature resistant surface insulation.
Embodiment 2
[0016] Embodiment 2. The preparation method provided by the present invention is as follows: firstly, rinse the FeCrAl electrothermal alloy product after degreasing and rust removal treatment; secondly, immerse the rinsed product in the sol-gel body containing rare earth for about 20 minutes Then take it out and dry it; finally heat treatment at 850-950°C in a protective atmosphere for about 120 minutes to obtain a FeCrAl electric heating alloy product with high temperature resistant surface insulation.
Embodiment 3
[0017] Embodiment 3. The preparation method provided by the present invention is as follows: firstly, rinse the FeCrAl electrothermal alloy product after degreasing and derusting treatment; secondly, immerse the rinsed product in a solution containing 1-5% hydrated aluminum hydroxide, 5 / 10,000 cerium-containing rare earth compound sol-gel body, take it out and dry it after about 16 minutes; finally heat treatment at 850-950°C in a protective atmosphere for about 160 minutes to obtain a high temperature resistant surface insulation FeCrAl electric heating alloy products.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
electrical resistance | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com