Pulverized coal activator and coking coal prepared from same

An activator and pulverized coal technology, which is applied in the field of pulverized coal activator and coking coal, can solve the problems of increased coal water content, unfavorable coke quality, and large dosage, so as to achieve increased fluidity and low overall cost , Improve the effect of fluidity

Inactive Publication Date: 2010-05-12
重庆汉砧科技有限公司
View PDF0 Cites 8 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Existing activators are generally composed of water-soluble polymer compounds, surfactants, salts, etc. During application, some of them are sprayed into blended coal through aqueous solution, which will increase the water content of coal, which is not conducive to coking, and the blending The input is large, the cost is high, and the sulfur content is too high, which is not conducive to the improvement of coke quality

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0037] Prepare coal powder activator, the weight percent of each component is: 3% resin clay, 6% glucose, 5% cobalt molybdate, 1% cholesterol benzoate, 2% boric anhydride, 3% Clay, 13% titanium dioxide, 16% sodium stearate, 2% ferric chloride, 9% clay, 3% anhydrous borax, 13% modified starch, 24% tar residue.

[0038] Then the pulverized coal activator is mixed with blended coal, wherein the weight percentage of the pulverized coal activator is 1%; the non-coking coal is lean coal, and the weight percentage is 20%; the coking blended coal weight percentage is 79%, and the proportioning is : Coking coal 25%, fat coal 20%, gas coal 15%, lean coal 40%. All kinds of coal are domestic coal.

Embodiment 2

[0040] Prepare coal powder activator, the weight percent of each component is: 12% resin clay, 23% glucose, 3% cobalt molybdate, 18% cholesterol benzoate, 28% boric anhydride, 2% Clay, 3% titanium dioxide, 2% sodium stearate, 1% ferric chloride, 2% clay, 3% anhydrous borax, 1% modified starch, 2% tar residue.

[0041] Then the pulverized coal activator is mixed with blended coal, wherein the weight percentage of the pulverized coal activator is 2%; the non-coking coal is white coal, and the weight percentage is 50%; the coking blended coal weight percentage is 48%, and the proportion is : Coking coal 25%, fat coal 20%, gas coal 15%, lean coal 40%. All kinds of coal are domestic coal.

Embodiment 3

[0043] Prepare coal powder activator, the weight percent of each component is: 5% resin clay, 10% glucose, 4% cobalt molybdate, 5% cholesterol benzoate, 18% boric anhydride, 8% Clay, 10% titanium dioxide, 4% sodium stearate, 2% ferric chloride, 4% clay, 18% anhydrous borax, 3% modified starch, 9% tar residue.

[0044] Then the pulverized coal activator is mixed with blended coal, wherein the weight percentage of the pulverized coal activator is 4%; the non-coking coal is non-caking coal, and the weight percentage is 75%; the coking blended coal weight percentage is 21%, and the proportion For: coking coal 25%, fat coal 20%, gas coal 15%, lean coal 40%. All kinds of coal are domestic coal.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention provides a pulverized coal activator, which comprises the following components in percentage by weight: 1 to 14 percent of resin clay, 5 to 26 percent of glucose, 0.5 to 5 percent of cobalt molybdate, 0.5 to 29 percent of cholesterol ester benzoate, 1 to 29 percent of boron anhydrous, 1 to 15 percent of clay, 1 to 15 percent of titanium dioxide, 1 to 17 percent of sodium stearate, 1 to 5 percent of ferric chloride, 1 to 10 percent of argil, 1 to 26 percent of anhydrous borax, 1 to 16 percent of modified starch , and 1 to 25 percent of tar residue. The pulverized coal activator added can be directly mixed with matched coal so as to ensure that active components and inert components of the matched coal can be easier to combine together during carbonization and raise the anisotropic tissue content of coke. The increase in coal fluidity is beneficial to intermediate phase for forming staged molecular rearrangement, promotes the transformation process of the intermediate phase, and forms higher-strength coke capable of replacing or partially replacing coking coal for coking. The pulverized coal activator has the advantages of small adding dose, high benefit and low comprehensive cost.

Description

technical field [0001] The invention relates to the field of coking coal blending, in particular to a pulverized coal activator and coal for coking prepared by the pulverized coal activator. Background technique [0002] Coke is an important raw material and fuel in the metallurgical industry. With the rapid development of my country's steel industry and the rapid growth of steel production, the demand for coke is increasing, and the quality requirements are also getting higher and higher. The quality of coke is seriously restricted by the shortage of coking coal resources in my country. Therefore, it is very urgent to develop non-coking coal to replace or partially replace coking coal for coking, especially for our country and has important strategic significance. [0003] Although my country's coal resources are abundant, there are not many types of coal suitable for coking, and the regional distribution of resources is extremely uneven. In particular, the reserves of hig...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C10B57/06
Inventor 傅勇邓先永
Owner 重庆汉砧科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products