Preparation method for trapping agent for bauxite flotation
A collector and bauxite technology, used in flotation, solid separation and other directions, can solve the corrosion of stainless steel equipment and other problems, and achieve the effect of reducing corrosion, reducing chloride ions, and strong collection ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0012] A method for preparing a collector for bauxite flotation, adding caustic soda solution, hydroxylamine sulfate solution and methyl benzoate in a ratio of 2:1.2:1 into a reaction kettle equipped with a cooling water cooling device, at a temperature of 50 Carry out the hydroximation reaction at ~60°C for 6-8 hours to obtain a mixed solution containing sodium benzohydroxamate, sodium sulfate, methanol and water, and then transfer the mixed solution to the dilution tank, and press the mixing button in the dilution tank at the same time The dilution ratio of the solution to water is 1:4, add demineralized water and stir well, then send the obtained solution into the storage tank.
[0013] Below in conjunction with example the present invention will be further described.
Embodiment 1
[0015] Feed caustic soda, hydroxylamine sulfate, and methyl benzoate at a ratio of 2:1.2:1, control the reaction temperature at 60°C, cool down with cooling water, react for 6 hours to form a white milky mixture, and add this mixture at a dilution ratio of 1:4 Dilute with demineralized water to obtain the intermediate product benzhydroxamate solution. The KL collector is obtained by blending the intermediate product with oleic acid and surfactant in a certain proportion.
[0016] Al-Si ratio 4.35, AI 2 o 3 Content 60.20%, SiO 2 The bauxite raw ore with a content of 13.83% was ground with a ball mill for 5 minutes, and the grinding fineness was -0.074mm, which accounted for 75%. The flotation test was carried out in the laboratory with a small flotation machine through one roughing and one sweeping. Add the prepared KL collector according to the roughing addition of 800g / ton raw ore and the sweeping addition of 200g / ton raw ore.
[0017] Beneficiation index: aluminum-silic...
Embodiment 2
[0019] Feed caustic soda, hydroxylamine sulfate, and methyl benzoate at a ratio of 2:1.2:1, control the reaction temperature at 50°C, cool down with cooling water, react for 6 hours to form a white milky mixture, and add this mixture at a dilution ratio of 1:4 Dilute with demineralized water to obtain the intermediate product benzhydroxamate solution. The KL collector is obtained by blending the intermediate product with oleic acid and surfactant in a certain proportion.
[0020] Al-Si ratio 4.35, AI 2 o 3 Content 60.20%, SiO 2 The bauxite raw ore with a content of 13.83% was ground with a ball mill for 5 minutes, and the grinding fineness was -0.074mm, accounting for 75%. The flotation test was carried out in the laboratory with a small flotation machine through one roughing and one sweeping. Add the prepared KL collector according to the roughing addition of 800g / ton raw ore and the sweeping addition of 200g / ton raw ore.
[0021] Beneficiation index: aluminum-silicon ra...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com