[0023] Embodiment 1: the bleaching method of this Dalong bamboo chemical pulp, specific content is as follows:
[0024] In the embodiment, the Dalong bamboo chemical pulp is made of Dalong bamboo as a raw material, which is split into bamboo chips with a length of 15mm, a thickness of 3mm, and a width of 20mm; It is: liquid ratio 1:4.5, alkali amount 22% (calculated as NaOH), degree of sulfidation 22%, after idling the cooking pot for 10 minutes, it takes 45 minutes to raise the temperature from the initial temperature to 100°C, and then it takes 120 minutes to rise to 165°C, and at 165°C ℃ for 120min. After cooking, the bamboo chips are decomposed into fibers and placed in a 300-mesh nylon mesh pulp bag, washed with clean water until the washing water becomes clear and free of foam, and then the bamboo pulp fibers are screened with a sieve machine to extract the fiber raw materials for bleaching. The Dalong bamboo pulp with a Kappa value of 14.2 and a viscosity of 1220 enter...
Embodiment 2
[0033] Embodiment 2: the bleaching method of this Dalong bamboo chemical pulp, specific content is as follows:
[0034] In the embodiment, the Dalong bamboo chemical pulp is made of Dalong bamboo as a raw material, split into bamboo chips with a length of 15 mm, a thickness of 3 mm, and a width of 20 mm; the bamboo chips are screened and cooked in a ZQL electric cooking pot by the caustic soda method-anthraquinone method , the cooking conditions are: liquid ratio 1:4, alkali amount 20% (calculated as NaOH), and then add anthraquinone of 0.10% dry weight of the pulp. After the cooking pot is idling for 10 minutes, it takes 30 minutes to raise the temperature from the initial temperature to 85 ℃, and then Rise to 165°C over 70 minutes and keep at 165°C for 150 minutes. After cooking, the bamboo chips are decomposed into fibers and placed in a 300-mesh nylon mesh pulp bag, washed with clean water until the washing water becomes clear and free of foam, and then the bamboo pulp fiber...
Embodiment 3
[0043] Embodiment 3: the bleaching method of this Dalong bamboo chemical pulp, specific content is as follows:
[0044] In the embodiment, Dalong bamboo chemical pulp is made of Dalong bamboo as raw material, split into bamboo chips with a length of 15 mm, a thickness of 3 mm, and a width of 20 mm; The conditions are: liquid ratio 1:4, adding 18% ammonium sulfite, 5% urea and 0.15% anthraquinone in absolute dry mass of pulp, idling the cooking pot for 10 minutes, then raising the temperature from the initial temperature to 150°C for 140 minutes, and heating at 150 ℃ for 60 minutes, and then raised to 165 ℃ in 20 minutes, and kept at 165 ℃ for 120 minutes. After cooking, the bamboo chips are decomposed into fibers and placed in a 300-mesh nylon mesh pulp bag, washed with clean water until the washing water becomes clear and free of foam, and then the bamboo pulp fibers are screened with a sieve machine to extract the fiber raw materials for bleaching. The Dalong bamboo pulp wi...
PUM
Property | Measurement | Unit |
---|---|---|
width | aaaaa | aaaaa |
whiteness | aaaaa | aaaaa |
whiteness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com