Woody ergosterol preparation method
An ergosterol and woody technology, applied in the field of preparation of woody ergosterol, can solve problems such as abandonment or burning, waste of biomass resources, environmental pollution, etc., achieves low production cost, realizes maximum utilization, and improves commercial value Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A preparation method of woody ergosterol, comprising the following steps:
[0018] (1) Extraction: According to the volume ratio V 木本原料 :V 混合溶剂 =1:0.3, mix the woody raw material with the mixed solvent, extract at a temperature of 70°C and normal pressure for 6.5 hours, then filter with seven layers of fine gauze to obtain the filtrate I; wherein the woody raw material refers to eucalyptus wood powder or camellia oleifera Shell powder; the mixed solvent is composed of benzene and petroleum ether according to the volume ratio V 苯 :V 石油醚 = 1:1 uniformly mixed organic solvent, the boiling point of petroleum ether used is 40°C;
[0019] (2) Concentration: at a vacuum of 0.04 MPa and a temperature of 45° C., the mixed solvent in the filtrate I is recovered to obtain a woody extract;
[0020] (3) cracking: according to the mass ratio m 木本抽提物 :m 催化剂 =1000:0.2, using woody extracts and catalysts to mix evenly, then thermally cracking in helium at 500°C for 40 minutes, and...
Embodiment 2
[0025] A preparation method of woody ergosterol, comprising the following steps:
[0026] (1) Extraction: According to the volume ratio V 木本原料 :V 混合溶剂 =1:0.7, mix the woody raw material with the mixed solvent, extract at a temperature of 75°C and normal pressure for 6.0 hours, then filter with seven layers of fine gauze to obtain the filtrate I; wherein the woody raw material refers to eucalyptus wood powder or camellia oleifera Shell powder; the mixed solvent is composed of benzene and petroleum ether according to the volume ratio V 苯 :V 石油醚 = 1:2 uniformly mixed organic solvent, the boiling point of petroleum ether used is 50°C;
[0027] (2) Concentration: at a vacuum of 0.04 MPa and a temperature of 40° C., the mixed solvent in the filtrate I is recovered to obtain a woody extract;
[0028] (3) cracking: according to the mass ratio m 木本抽提物 :m 催化剂 =1000:0.3, using woody extracts and catalysts to mix evenly, then thermally cracking in helium at 550°C for 20 minutes, and...
Embodiment 3
[0033] A preparation method of woody ergosterol, comprising the following steps:
[0034] (1) Extraction: According to the volume ratio V 木本原料 :V 混合溶剂 =1:1.0, mix the woody raw material with the mixed solvent, extract at a temperature of 80°C and normal pressure for 5.5 hours, then filter with seven layers of fine gauze to obtain the filtrate I; wherein the woody raw material refers to eucalyptus wood powder or camellia oleifera fruit Shell powder; the mixed solvent is composed of benzene and petroleum ether according to the volume ratio V 苯 :V 石油醚 =1:4 organic solvent uniformly mixed, the boiling point of petroleum ether used is 60°C;
[0035] (2) Concentration: under a vacuum of 0.06MPa and a temperature of 50°C, the mixed solvent in the filtrate I is recovered to obtain the woody extract;
[0036] (3) cracking: according to the mass ratio m 木本抽提物 :m 催化剂 =1000:0.4, using woody extracts and catalysts to mix evenly, then thermally cracking in helium at 550°C for 30 minut...
PUM
| Property | Measurement | Unit |
|---|---|---|
| boiling point | aaaaa | aaaaa |
| boiling point | aaaaa | aaaaa |
| boiling point | aaaaa | aaaaa |
Abstract
Description
Claims