Embodiment 1
[0044] The proportioning that immobilization reagent adopts is: by the potassium dihydrogen phosphate of 18 (weight) %, the sodium sulfide of 27 (weight) %, the calcium oxide of 44.5 (weight) %, the calcium carbonate of 10 (weight) %, 0.3 ( (weight) % calcium type A molecular sieve and 0.2 (weight) % disodium edetate.
[0045] The immobilization treatment steps adopted are as follows:
[0046] (1) First weigh the components for preparing 1 part by weight of immobilization reagent according to the following proportions: 18 (weight) % potassium dihydrogen phosphate, 27 (weight) % sodium sulfide, 44.5 (weight) % calcium oxide , 10 (weight)% calcium carbonate, 0.3 (weight)% calcium type A molecular sieve and 0.2 (weight)% disodium edetate;
[0047] (2) Weigh 20 weight samples of heavy metal pollutants;
[0048] (3) Stir and mix the metal oxide, strong base and weak salt compound, metal stabilizer and metal chelating agent weighed in step (1) evenly, and use it as reagent A for l...
Embodiment 2
[0057] The proportioning that immobilization reagent adopts is: by the calcium hydrogen phosphate of 24.5 (weight)%, the sodium sulfide of 8 (weight)%, the calcium oxide of 42 (weight)%, the calcium carbonate of 25 (weight)%, 0.1 (weight) )% of sodium molecular sieve type A and 0.4% by weight of disodium edetate.
[0058] The immobilization treatment steps adopted are as follows:
[0059] (1) First weigh the components for preparing 1 part by weight of immobilization reagent according to the following proportions: 24.5 (weight) % calcium hydrogen phosphate, 8 (weight) % sodium sulfide, 42 (weight) % calcium oxide, 25 (weight) % calcium carbonate, 0.1 (weight) % sodium type A molecular sieve and 0.4 (weight) % disodium edetate;
[0060] (2) Weigh 20 weight samples of heavy metal pollutants;
[0061] (3) Stir and mix the metal oxide, strong base and weak salt compound, metal stabilizer and metal chelating agent weighed in step (1) evenly, and use it as reagent A for later use;...
Embodiment 3
[0070] The proportioning that immobilization reagent adopts is: by the calcium dihydrogen phosphate of 25 (weight) %, the calcium sulfide of 8 (weight) %, the calcium oxide of 42 (weight) %, the calcium carbonate of 24.5 (weight) %, 0.4 ( % by weight of sodium type A molecular sieve and 0.1 % by weight of disodium edetate.
[0071] The immobilization treatment steps adopted are as follows:
[0072] (1) First, weigh and prepare 1 part of immobilization reagent according to the following proportions: 25 (weight) % calcium dihydrogen phosphate, 8 (weight) % calcium sulfide, 42 (weight) % calcium oxide, 24.5% by weight calcium carbonate, 0.4% by weight sodium type A molecular sieve and 0.1% by weight disodium edetate;
[0073] (2) Weigh 40 weight samples of heavy metal pollutants;
[0074] (3) Stir and mix the metal oxide, strong base and weak salt compound, metal stabilizer and metal chelating agent weighed in step (1) evenly, and use it as reagent A for later use;
[0075] (4...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com