Method for preparing halamine antibacterial material based on cyanuric chloride
An antibacterial material, cyanuric chloride technology, applied in the field of antibacterial materials, can solve problems such as increased finishing costs, textile strength loss, harsh reaction conditions, etc., and achieve high raw material utilization, excellent antibacterial performance, and mild process conditions.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Completely dissolve 1g of cyanuric chloride and 2g of sodium hydroxide in 97g of distilled water to prepare a finishing solution, and then soak the natural fiber textiles (pure cotton fabric, purchased from Zhejiang Guandong Printing and Dyeing Garment Co., Ltd.) in the finishing solution for 15 minutes. , Two dipping and two rolling, the residual rate is 100%; after finishing, take it out and put it in a dryer at 80℃ for 5min, then put it in a dryer at 120℃ for 10min; take out the fabric with a mass concentration of 0.5 Wash the surface with 5% standard soap flake solution and a large amount of deionized water and dry at room temperature; soak the dried fabric in a calcium hypochlorite solution with a concentration of 0.01% by mass (adjust the pH to 7.0 with dilute sulfuric acid) After 1h, the fabric was taken out and washed with a large amount of water, and dried in a dryer at 45℃ for 2h to obtain an antibacterial cotton fabric. The available chlorine content of the an...
Embodiment 2
[0027] 8g of cyanuric chloride and 7g of potassium hydroxide were completely dissolved in 87g of distilled water to prepare a finishing solution, and then natural fiber textiles (pure cotton fabric, purchased from Zhejiang Guandong Printing and Dyeing Garment Co., Ltd.) to be finished were soaked in the finishing solution for 15 minutes , Two soaking and two rolling, the residual rate is 100%; after finishing, take it out and put it in a dryer at 80℃ for 5min, then put it in a dryer at 90℃ for 40min; take out the fabric with a mass concentration of 0.5 Wash the surface with 5% standard soap flake solution and a large amount of deionized water, and dry at room temperature; soak the dried fabric in a sodium hypochlorite solution with a concentration of 0.5% by mass (adjust the pH value to 12.0 with dilute sulfuric acid), after 1 hour The fabric was taken out and washed with a large amount of water, and dried in a dryer at 45°C for 2 hours to obtain an antibacterial cotton fabric. ...
Embodiment 3
[0029] 5g of cyanuric chloride and 11g of potassium hydroxide were completely dissolved in 84g of distilled water to prepare a finishing solution, and then natural fiber textiles (pure cotton fabrics, purchased from Zhejiang Guandong Printing and Dyeing Garment Co., Ltd.) to be finished were soaked in the finishing solution for 15 minutes , Two soaking and two rolling, the residual rate is 100%; after finishing, take it out and put it in a dryer at 80℃ for 5min, then put it in a dryer at 100℃ for 20min; take out the fabric with a mass concentration of 0.5 Wash the surface with 5% standard soap flake solution and a large amount of deionized water, and dry it at room temperature; soak the dried fabric in a sodium hypochlorite solution with a concentration of 0.1% by mass (adjust the pH to 7.0 with dilute sulfuric acid), after 1 hour The fabric was taken out and washed with a large amount of water, and dried in a dryer at 45°C for 2 hours to obtain an antibacterial cotton fabric. ...
PUM
Login to View More Abstract
Description
Claims
Application Information