Wood drying method for solid wood furniture

A wood and furniture technology, used in drying, drying solid materials, heating to dry solid materials, etc., can solve the problems of not being directly exposed to sunlight, not being too cold and overheating, difficult maintenance, etc., to eliminate internal stress and woodiness. , the effect of accelerated dehumidification and long service life

Inactive Publication Date: 2013-07-17
天津福通木业有限公司
View PDF3 Cites 13 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] However, the main disadvantage of solid wood furniture is that it is easy to deform, and it is difficult to maintain. For example, it cannot be exposed to direct sunlight, it cannot be too cold or too hot, and the environment that is too dry and humid is not suitable for solid wood furniture; Air conditioning causes excessive temperature and humidity changes, so the wood drying step before solid wood furniture is particularly important

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0030] A wood drying method for solid wood furniture. In this embodiment, birch is taken as an example, and the birch is made into a plurality of wet boards (that is, log boards) with a length of 2000mm---4000mm, a width of 60mm, and a thickness of 25mm. Its drying steps are:

[0031] ⑴One-time drying treatment: stack the wet birch boards in the drying kiln for air-drying, close the dehumidification window, raise the temperature in the kiln to 65°C, and keep the humidity in the kiln at 62%~65%. After 3 hours, adjust The temperature in the kiln is 55°C, and the humidity in the kiln is kept above 45%. After 2 hours, open the dehumidification window, adjust the humidity in the kiln to below 48%, keep it at room temperature for 30-50 hours, and carry out the second drying treatment ;

[0032] ⑵Secondary drying treatment: close the dehumidification window, raise the temperature in the kiln to 65°C, and keep the humidity in the kiln at 61%~63%. After 5 hours, adjust the temperature...

Embodiment 2

[0040] A wood drying method for solid wood furniture. In this embodiment, oak wood is taken as an example, and the oak wood is made into a plurality of wet boards with a length of 2000mm---4000mm, a width of 60mm, and a thickness of 25mm. The steps are:

[0041] ⑴ One-time drying treatment: stack the wet oak boards in the drying kiln for air-drying, close the dehumidification window, raise the temperature in the kiln to 65°C, and keep the humidity in the kiln at 62%~64%. After 3 hours, Adjust the temperature in the kiln to 55°C, and keep the humidity in the kiln above 45%. After 2 hours, open the dehumidification window, adjust the humidity in the kiln to below 48%, keep it at room temperature for 30-50 hours, and carry out secondary drying deal with;

[0042] (2) Secondary drying treatment: close the dehumidification window, raise the temperature in the kiln to 65°C, and keep the humidity in the kiln at 62%~64%. After 5 hours, adjust the temperature in the kiln to 58°C, and ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to a wood drying method for solid wood furniture. The method comprises the steps of stacking drying piles of wet wood plates in a drying kiln, performing warming and humidifying drying processing for five times, performing maintenance for 48 h after kiln stopping, and obtaining finished products. The moisture content of dried wood plates obtained through the drying method is merely 8%-10%, inherent strain of wood is extremely small, and the dried wood plates are long in service lives and moisture-resistant, cannot deform easily and can be over five times as strong as ordinary plate type furniture in deformation resistance. According to the drying method, the wood undergoes about 240-hour steam drying and undergoes humidifying processing for four times, and temperature of the wood is improved step by step, so that elimination of the inherent strain and nature of the wood is accelerated, and high standard for manufacturing the furniture is met.

Description

technical field [0001] The invention belongs to the field of drying technology, in particular to a wood drying method for solid wood furniture. Background technique [0002] Solid wood furniture is made of solid wood sawn lumber or solid wood board as the base material, and the surface is treated as furniture, or the furniture that is coated with solid wood veneer or veneer (wood veneer) on such a base material . Commonly used wood for solid wood furniture includes mahogany, teak, mahogany, walnut wood, crabapple wood, ash, northeast elm, eucalyptus, camphor wood, basswood, birch, colored wood, beech, cherry wood, rosewood, cypress , yew, Korean pine, oak wood, yellow pineapple, walnut catalpa, Schima superba, rosewood, neem, red toon, wild jujube, etc. [0003] Solid wood furniture is natural, environmentally friendly, and healthy. Log-colored furniture is natural and free from chemical pollution. It is not only the best choice for modern healthy life, but also meets the ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): F26B3/02
Inventor 赵维强
Owner 天津福通木业有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products