Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Coated wood made of cedar wood

A raw material and wood technology, applied in wood treatment, humidity control wood, wood processing appliances, etc., can solve problems such as damage to precious tree species or wild wood, insufficient economic value, poor paint and bonding performance, etc., and achieve waterproof effect. Good, increase the scope of application, the effect of smooth and delicate appearance

Inactive Publication Date: 2015-11-04
重庆家和琴森木业有限公司
View PDF8 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Due to the well-developed resin pipe diameter of cedar cedar, high oil content, large deformation of wood, serious warping and cracking when dry, not resistant to corrosion, even overflowing oil and contaminating the surface of the material when the temperature is high, resulting in poor paint and bonding performance; The texture of fir is obvious, and the color of early wood and late wood is inconsistent, so that it is difficult to cover with water-based paint, which affects the quality of wood products, so it is rarely used in furniture. At present, it is mainly used for building templates, ore pillars, boards, packing boxes, and matches. Rods, plywood, etc., or as a raw material for man-made fiberboard
[0003] However, as a kind of fast-growing economic forest, cedar is widely planted in most mountainous areas of our country. Due to the limitation of its application field, its due economic value is not fully exerted; it indirectly causes the destruction of other precious tree species or wild wood

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Coated wood made of cedar wood

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] First, the cedar wood is cut and sawed into a length of 100cm and a thickness of 2cm; then the temperature in the conventional steam drying kiln is adjusted at 68°C, and water vapor is sprayed in the conventional steam drying kiln to make it saturated, and then the cedar is Put the wood and wood trim into the conventional steam drying kiln to fully absorb water. After 25 hours, the cedar wood absorbs water to reach saturation, then stop spraying water vapor, adjust the temperature in the conventional steam drying kiln at 63°C, and keep the kiln for 12 hours, then start Exhaust the vent hole outward, and gradually raise the temperature inside the conventional steam drying kiln to 82°C, and dehydrate for 4 hours; repeat this twice, and then check the moisture content of the wood until the moisture content is between 8-10%. Obtain dry cedar wood and its offcuts.

[0019] Then batching, coarsely processing the dried cedar wood edge material into 1-10 purpose coarse wood pow...

Embodiment 2

[0022] Firstly, the cedar wood is cut and sawed into lumber with a length of 200cm and a thickness of 5cm; then the temperature in the conventional steam drying kiln is adjusted at 70°C, and water vapor is sprayed into the conventional steam drying kiln to make it saturated, and then the degreased Put the cedar wood and wood side materials into the conventional steam drying kiln to fully absorb water. After 28 hours, the cedar wood absorbs water to reach saturation, then stop spraying water steam, adjust the temperature in the conventional steam drying kiln at 65 ° C, and keep the kiln for 14 hours. , and then open the exhaust hole to exhaust outside, and gradually raise the temperature in the conventional steam drying kiln to 85°C, and dehydrate for 5 hours; repeat this 4 times, and then check the moisture content of the wood until the moisture content is 8-10% , to obtain dry cedar wood and its offcuts.

[0023] Then batching, coarsely processing the dried cedar wood edge ma...

Embodiment 3

[0026] Firstly, the cedar wood is cut and sawed into lumber with a length of 300cm and a thickness of 6cm; then the temperature in the conventional steam drying kiln is adjusted at 72°C, and water vapor is sprayed into the conventional steam drying kiln to make it saturated, and then the degreased Put the cedar wood and wood side materials into the conventional steam drying kiln to fully absorb water. After 30 hours, the cedar wood absorbs water to reach saturation, then stop spraying water steam, adjust the temperature in the conventional steam drying kiln at 67 ° C, and keep the kiln for 15 hours , and then open the exhaust hole to exhaust outside, and gradually raise the temperature in the conventional steam drying kiln to 87°C, and dehydrate for 6 hours; repeat this 4 times, and then check the moisture content of the wood until the moisture content is 8-10% , to obtain dry cedar wood and its offcuts.

[0027] Then batching, coarsely processing the dried cedar wood edge mat...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle sizeaaaaaaaaaa
particle sizeaaaaaaaaaa
Login to View More

Abstract

Coating timber with Japan cedar wood as a raw material belongs to the technical field of wood plate production. The coating timber is produced through eight procedures, including, drying, material preparing, sanding, repairing, coating, re-coating, re-sanding and painting. The beneficial effects are that: the ultrafine Japan timber powder is used as the main raw material to repair the timber and serves as a contact medium of the timber and the coating, so that the coating material and the Japan cedar timber can be fully and easily integrated; the coating material is made into a primary coating material and a repeated coating material according to two proportions, the primary coating material controls the expansion of the annual rings, and the repeated coating material can enable the coating timber to keep the outer surface smooth and fine; the examination shows that the coating timber with the Japan cedar wood as the raw material has a fine and compact coating texture, strong flame retardancy, uniform coating, a strong anti-compact capability and a good waterproof effect, so that performances of the Japan cedar timber are not only improved, the application range of the Japan cedar timber is also increased greatly; the deserved economic value of the Japan cedar timber can be fully played, and conditions are created for the protection of the wild wood and forests.

Description

technical field [0001] The invention belongs to the technical field of wood board production, in particular to a coated wood material using cedar wood as a raw material. Background technique [0002] Due to the well-developed resin pipe diameter of cedar cedar, high oil content, large deformation of wood, serious warping and cracking during drying, and no corrosion resistance, when the temperature is high, it even spills oil and contaminates the surface of the material, resulting in poor paint and bonding performance; The texture of fir is obvious, and the color of early wood and late wood is inconsistent, so that it is difficult to cover with water-based paint, which affects the quality of wood products, so it is rarely used in furniture. At present, it is mainly used for building templates, ore pillars, boards, packing boxes, and matches. Rods, plywood, etc., or as a raw material for man-made fiberboards. [0003] But cedar, as a kind of fast-growing economic forest, is w...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): B27M3/08B27K1/00B27G1/00B27K5/00
Inventor 杨琴
Owner 重庆家和琴森木业有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products