Sound absorption material
A sound-absorbing material, octyl phenolic resin technology, applied in the field of sound-absorbing materials, can solve the problems of poor sound-absorbing characteristics, large base material volume, and poor constructability, and achieve fast setting speed, small base material volume, and excellent constructability Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] The sound-absorbing material provided by the present invention comprises the following parts by weight: 8 parts of octylphenolic resin, 0.9 part of stearic acid, 23 parts of carbon powder, 78 parts of talcum powder, 10 parts of vermiculite powder, 0.6 parts of tin, 12 parts of dibutyl phthalate, 2.6 parts of composite sol, 8.8 parts of inorganic fiber, 1 part of rare earth oxide, 1 part of zirconia, 1 part of surfactant, 1 part of aluminate cement, PVA aqueous solution 7 servings.
Embodiment 2
[0018] The sound-absorbing material provided by the present invention comprises the following parts by weight: 10 parts of octylphenolic resin, 1 part of stearic acid, 30 parts of carbon powder, 80 parts of talcum powder, 15 parts of vermiculite powder, 1.5 parts of tin, 15 parts of dibutyl phthalate, 16 parts of composite sol, 15 parts of inorganic fiber, 3 parts of rare earth oxide, 1.5 parts of zirconia, 0.3 parts of surfactant, 3 parts of aluminate cement, PVA aqueous solution 24 servings.
Embodiment 3
[0020] The sound-absorbing material provided by the present invention comprises the following parts by weight: 13 parts of octylphenolic resin, 2.3 parts of stearic acid, 35 parts of carbon powder, 85 parts of talcum powder, 18 parts of vermiculite powder, 1.8 parts of tin, 19 parts of dibutyl phthalate, 30 parts of composite sol, 30 parts of inorganic fiber, 6 parts of rare earth oxide, 2.5 parts of zirconia, 0.6 part of surfactant, 5.5 parts of aluminate cement, PVA aqueous solution 36 servings.
[0021] The preparation method of the sound-absorbing material is characterized in that it comprises the following steps:
[0022] First mix octyl phenolic resin, stearic acid, composite sol, and PVA aqueous solution, then stir in the internal mixer for 10-20 minutes, then add carbon powder, talc powder, vermiculite powder, stannous chloride, diphthalate Butyl ester, inorganic fiber, rare earth oxide, zirconia, surfactant, aluminate cement, and continue to stir for 20-30 minutes to...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com