[0011] This embodiment provides a coating for protecting exterior walls, which contains the following components in parts by mass: 11.5 parts of silicone acrylic resin, 3 parts of silicone oil, 0.5 part of protective glue, 1 part of polyoxyethylene stearate, lauryl 0.7 parts of sodium benzenesulfonate, 0.2 parts of lauroyl peroxide, 0.08 parts of sodium bicarbonate, 1.5 parts of low-wax pitch, 0.1 part of lauryl alcohol ester, 0.5 part of ethyl acetate, and 15 parts of deionized water.
[0012] The preparation steps of a coating for protecting exterior walls are as follows: add polyoxyethylene stearate, deionized water, sodium bicarbonate, silicone acrylic resin and lauroyl peroxide in a reaction kettle, stir and mix for 0.5h, and heat up to 80 ℃, add silicone oil, protective glue, sodium dodecylbenzenesulfonate, lauryl alcohol ester, mix well, and finally add low-wax asphalt and ethyl acetate, keep the temperature at 80 ℃, keep it warm for 2 hours, and then lower it to room te...
Embodiment 2
[0014] This embodiment provides a coating for protecting exterior walls, which contains the following components in parts by mass: 14 parts of silicone acrylic resin, 4 parts of silicone oil, 0.8 parts of protective glue, 1.5 parts of polyoxyethylene stearate, lauryl 1 part of sodium benzenesulfonate, 0.27 part of lauroyl peroxide, 0.1 part of sodium bicarbonate, 2 parts of low-wax pitch, 0.15 part of lauryl alcohol ester, 0.7 part of ethyl acetate, 20 parts of deionized water.
[0015] The preparation steps of a coating for protecting exterior walls are as follows: add polyoxyethylene stearate, deionized water, sodium bicarbonate, silicone acrylic resin and lauroyl peroxide in a reaction kettle, stir and mix for 0.5h, and heat up to 90 ℃, add silicone oil, protective glue, sodium dodecylbenzenesulfonate, lauryl alcohol ester, mix well, and finally add low-wax asphalt and ethyl acetate, keep the temperature at 90 ℃, keep it warm for 2 hours, and then lower it to room temperatur...
Embodiment 3
[0017] This embodiment provides a coating for protecting exterior walls, which contains the following components in parts by mass: 20 parts of silicone acrylic resin, 5 parts of silicone oil, 1.2 parts of protective glue, 3 parts of polyoxyethylene stearate, lauryl 1.3 parts of sodium benzenesulfonate, 0.4 parts of lauroyl peroxide, 0.12 parts of sodium bicarbonate, 3 parts of low-wax pitch, 0.25 parts of lauryl alcohol ester, 0.9 parts of ethyl acetate, and 25 parts of deionized water.
[0018] The preparation steps of a coating for protecting exterior walls are as follows: add polyoxyethylene stearate, deionized water, sodium bicarbonate, silicone acrylic resin and lauroyl peroxide in a reaction kettle, stir and mix for 0.5h, and heat up to 80 ℃, add silicone oil, protective glue, sodium dodecylbenzenesulfonate, lauryl alcohol ester, mix well, and finally add low-wax asphalt and ethyl acetate, keep the temperature at 80 ℃, keep it warm for 2 hours, and then lower it to room t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com