A technology of corrugated paper and moisture-proof agent, which is applied in the field of preparation of moisture-proof corrugated paper, can solve the problems of poor waterproof and moisture-proof ability, achieve the effects of low production cost, wide source of raw materials, and improved waterproof and moisture-proof performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] The preparation method of the moisture-proof corrugated paper in this example includes the following steps: Weigh 1 kg of wood pulp and 2 kg of waste paper pulp, mix them evenly, remove impurities, add 3.5 kg of water at a temperature of 35°C to soak the pulp for 15 minutes, and then transfer it to a disperser Disperse the pulp to obtain the original pulp; add 0.75 kg of moisture-proof agent to the original pulp, and make paper; preheat the paper, use a sizing machine to apply the adhesive evenly on the surface of the paper, and pass it through a single-facer to obtain corrugated paper. Paste a layer of waxed paper on the outermost layer of corrugated paper, and finally transfer it to an oven for drying.
[0021] In this embodiment, wood pulp is prepared from wood scraps.
[0022] The moistureproof agent in this example is prepared from the following raw materials in parts by weight: 25 parts of tapioca starch, 20 parts of styrene propylene, 15 parts of crotonate, 8 par...
Embodiment 2
[0024] The preparation method of the moisture-proof corrugated paper in this example includes the following steps: take 10 kg of wood pulp and 10 kg of waste paper pulp respectively, mix them evenly, remove impurities, add 25 kg of water with a temperature of 42°C to soak the pulp for 10 minutes, and then transfer it to a disperser Break up the pulp to obtain the original pulp; add 3.8 kg of moisture-proof agent to the original pulp, and make paper; preheat the paper, use a sizing machine to apply the adhesive evenly on the surface of the paper, and pass it through a single-facer to obtain corrugated paper. Paste a layer of waxed paper on the outermost layer of corrugated paper, and finally transfer it to an oven for drying.
[0025] The wood pulp in this example is prepared from wood scraps.
[0026] The moistureproof agent in this example is prepared from the following raw materials in parts by weight: 27 parts of tapioca starch, 15 parts of styrene propylene, 13 parts of cr...
Embodiment 3
[0028] The preparation method of the moisture-proof corrugated paper in this example includes the following steps: weigh 20 kg of wood pulp and 60 kg of waste paper pulp, mix them evenly, remove impurities, add 95 kg of water at a temperature of 50°C to soak the pulp for 13 minutes, and then transfer it to a disperser Disperse the pulp to obtain the original pulp; add 11.2 kg of moisture-proof agent to the original pulp, and make paper; preheat the paper, use a sizing machine to apply the adhesive evenly on the surface of the paper, and pass it through a single-sided machine to obtain corrugated paper. Paste a layer of waxed paper on the outermost layer of corrugated paper, and finally transfer it to an oven for drying.
[0029] The wood pulp in this example is prepared from wood scraps.
[0030] The moistureproof agent in this example is prepared from the following raw materials in parts by weight: 30 parts of tapioca starch, 17 parts of styrene propylene, 18 parts of crotona...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com