[0001] The invention relates to an anti-aging thermal insulation foam material. Background technique
[0002] Isotactic polypropylene is polypropylene with an isotactic structure. It is a highly crystalline thermoplastic resin with excellent rigidity and high temperature impact resistance.
[0003] Polypropylene (PP) foamed plastic products have good thermal stability (maximum service temperature up to 130°C) and good product dimensional stability at high temperatures, high toughness, tensile strength and impact strength, and excellent microwave adaptability It has attracted much attention due to its safety and environmental friendliness, thus becoming a good substitute for polystyrene (PS) foam plastics and polyurethane (PU) foam plastics. At present, polypropylene foam products are widely used in the field of food and food packaging, such as: trays, dishes, boxes, basins, beverage cups, sealed boxes and sealing gaskets for drinking water bottles, meat pack...
Examples
Embodiment 1
[0011] An anti-aging thermal insulation foam material, comprising the following parts by weight: 95 parts of isotactic polypropylene, 345 parts of stearic acid, 7 parts of carboxymethyl cellulose, 8 parts of polypropylene, 10 parts of organic montmorillonite, phosphate ester 7 parts, 40 parts of benzyl alcohol, 19 parts of Scherichia vine sawdust, 18 parts of cobalt naphthenate, 40 parts of oxalic acid, and 38 parts of Buna rubber.
Embodiment 2
[0013] An anti-aging thermal insulation foam material, comprising the following parts by weight: 80 parts of isotactic polypropylene, 33 parts of stearic acid, 1 part of carboxymethyl cellulose, 3 parts of polypropylene, 5 parts of organic montmorillonite, phosphoric acid ester 3 parts, 30 parts of benzyl alcohol, 15 parts of Scherichia chinensis sawdust, 11 parts of cobalt naphthenate, 21 parts of oxalic acid, 19 parts of Buna rubber.