Leather softening agent
A leather softener and polyether modification technology, which is applied in the field of leather treatment agents and leather softeners, can solve the problems of inability to harden and repair the interior of the leather, short durability, poor leather affinity, etc., to prolong life and rebound elasticity The effect of smoothness and good air permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Example 1 adopts the following raw materials in parts by weight: 22 parts of polyether-modified hydrophilic silicone oil, 18 parts of glycerol phosphate, 11 parts of sodium dodecyl sulfonate, 52 parts of ethanol, 8 parts of peregrine, 29 parts of water parts, 1 part of lemon essential oil, follow the steps below:
[0014] (1) Mix and disperse the polyether-modified hydrophilic silicone oil and glycerol phosphate at a speed of 1400 r / min for 12 minutes, and add one-fifth of water, one-third of equal weight, and one-third of ethanol. , continue to stir for 3min;
[0015] (2) Put the sodium dodecyl sulfonate, the remaining ethanol, and the remaining water in another disperser, mix and stir evenly, add the remaining peregrine and lemon essential oil, continue to stir for 5 minutes, and then add step (1) to prepare The mixed emulsion was stirred and dispersed for 5 minutes to obtain a leather softener.
Embodiment 2
[0016] Embodiment 2 adopts the following raw materials in parts by weight: 28 parts of polyether-modified hydrophilic silicone oil, 15 parts of glycerol phosphate, 10.5 parts of sodium dodecyl sulfonate, 55 parts of ethanol, 10.5 parts of peregrine, 30 parts of water ~50 parts, 3 parts of lemon essential oil, follow the steps below:
[0017] (1) Mix and disperse the polyether-modified hydrophilic silicone oil and glycerol phosphate at a speed of 1200 r / min for 15 minutes, and add one-fifth of water, one-third of equal weight, and one-third of ethanol. , continue to stir for 5min;
[0018] (2) Put the sodium dodecyl sulfonate, the remaining ethanol, and the remaining water in another disperser, mix and stir evenly, add the remaining peregrine and lemon essential oil, continue to stir for 6 minutes, and then add step (1) to prepare The mixed emulsion was stirred and dispersed for 5 minutes to obtain a leather softener.
Embodiment 3
[0019] Embodiment 3 adopts the following raw materials in parts by weight: 33 parts of hydrophilic silicone oil modified by polyether, 22 parts of glycerol phosphate, 20 parts of sodium dodecyl sulfonate, 60 parts of ethanol, 15 parts of peregrine, water 50 parts, 2 parts lemon essential oil, follow the steps below:
[0020] (1) Mix and disperse the polyether-modified hydrophilic silicone oil and glycerol phosphate at a speed of 1600 r / min for 10 minutes, and add one-fifth of water, one-third of equal weight, and one-third of ethanol. , continue to stir for 5min;
[0021] (2) Put the sodium dodecyl sulfonate, the remaining ethanol, and the remaining water in another disperser, mix and stir evenly, add the remaining peregrine and lemon essential oil, continue to stir for 8 minutes, and then add step (1) to prepare The mixed emulsion was stirred and dispersed for 5 minutes to obtain a leather softener.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com