Environment-friendly leather care agent
A kind of care agent and environment-friendly technology, applied in the field of leather care agent and environment-friendly leather care agent, it can solve the problems of oil volatilization, leather hardening, oil or oil film damage, etc., and achieve good repairing effect, smooth resilience, good The effect of air permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Embodiment 1 is made of the following raw materials in parts by weight: 15 parts of soybean oil, 10 parts of coconut oil, 10 parts of castor oil, 25 parts of polyether-modified hydrophilic silicone oil, 9 parts of organic silicone oil, 44 parts of polyethylene glycol, 12 parts of tetrapolypropylene benzene sulfonate sodium, 1.5 parts of rose essential oil, 0.5 part of brightener, adopt following steps to prepare a kind of environment-friendly type leather care agent: soybean oil, coconut oil, castor oil, organosilicon oil, macrogol 22 Parts were mixed evenly, and heated to 30°C, then placed under 30kHz ultrasonic waves for 5 minutes, added polyether-modified hydrophilic silicone oil, 6 parts of sodium tetrapolypropylene benzene sulfonate, and the remaining polyethylene glycol, and heated To 35°C, continue ultrasonic treatment at the same frequency for 3 minutes, then add the remaining tetrapolypropylene benzene sulfonate sodium, rose essential oil, brightener, Tween 80, ...
Embodiment 2
[0015] Example 2 The following raw materials in parts by weight: 12 parts of cottonseed oil, 10 parts of castor oil, 23 parts of coconut oil, 35 parts of polyether-modified hydrophilic silicone oil, 65 parts of silicone oil, 30 parts of polyethylene glycol, 10 parts of sodium tetrapolypropylene benzene sulfonate, 5 parts of Tween 80, and 1 part of brightener were prepared by the following steps: Mix vegetable oil, silicone oil, and polyethylene glycol 15 parts evenly, and heat to 35 ° C, and then place Ultrasonic treatment at 35kHz for 10min, add polyether-modified hydrophilic silicone oil, 5 parts of tetrapolypropylene benzene sulfonate sodium, and the remaining polyethylene glycol, raise the temperature to 40°C, and continue ultrasonic treatment at the same frequency After 5 minutes, add the remaining sodium tetrapropylene benzene sulfonate, brightener, and Tween 80, raise the temperature to 45°C, and continue ultrasonic treatment for 5 minutes at the same frequency.
Embodiment 3
[0016] Example 3 The following raw materials in parts by weight: 15 parts of soybean oil, 5 parts of coconut oil, 30 parts of polyether-modified hydrophilic silicone oil, 10 parts of silicone oil, 55 parts of polyethylene glycol, tetrapropylene benzene sulfonate 16 parts of sodium bicarbonate, 2 parts of Tween 80, and 2 parts of lemon essential oil were prepared by the following steps: Mix vegetable oil, silicone oil, and 27.5 parts of polyethylene glycol evenly, and heat to 30°C, and then place them under 25kHz ultrasonic waves Sonicate for 6 minutes, add polyether-modified hydrophilic silicone oil, 8 parts of sodium tetrapolypropylene benzene sulfonate, and the remaining polyethylene glycol, raise the temperature to 40 ° C, continue ultrasonic treatment for 3 minutes at the same frequency, and then add the remaining Sodium tetrapolypropylene benzene sulfonate, lemon essential oil, Tween 80, heated to 45 ° C, and continued ultrasonic treatment for 3 min at the same frequency. ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com