[0017] A method for spraying a protective layer on a metal surface, comprising the steps of:
[0018] (1) Mixing of raw materials: 15 parts by weight of o-phthalic unsaturated polyester resin, 25 parts of styrene, 5 parts of matte UV oil with a particle size of 15-25um, 8 parts of nylon fiber, and 12 parts of wollastonite , 2 parts of tert-butyl benzoate and 1 part of benzoyl peroxide are mixed evenly.
[0019] (2) Metal pretreatment: Clean the metal in an ultrasonic generator with dewaxing water for 3 minutes, soak it in hot pure water after cleaning it, and let it dry;
[0020] (3) Coating curing: the liquid coating is injected into the mold with a high-pressure automatic spray gun to control the vacuum degree to -0.06 Pa, and the mold is heated and kept at 165°C for curing under pressure;
[0021] (4) Spraying: The hardware surface that is evenly sprayed with paint is carried out at 90°C;
[0022] (5) Drying: Put the coated metal into an oven, control the temperature at 7...
Embodiment 2
[0024] A method for spraying a protective layer on a metal surface, comprising the steps of:
[0025] (1) Mixing of raw materials: 18 parts by weight of isophthalic unsaturated polyester resin, 25 parts of styrene, 6 parts of matte UV oil with a particle size of 15-25um, 10 parts of nylon fiber, and 15 parts of wollastonite , 4 parts of tert-butyl benzoate and 2 parts of benzoyl peroxide are mixed evenly.
[0026] (2) Metal pretreatment: Clean the metal in an ultrasonic generator with dewaxing water for 3 minutes, soak it in hot pure water after cleaning it, and let it dry;
[0027] (3) Coating curing: the liquid coating is injected into the mold with a high-pressure automatic spray gun to control the vacuum degree to -0.06 Pa, and the mold is heated and kept at 165°C for curing under pressure;
[0028] (4) Spraying: The hardware surface that is evenly sprayed with paint is carried out at 90°C;
[0029] (5) Drying: put the coated metal into an oven, control the temperature a...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com