[0026] Select pure cotton fabric, the warp and weft densities are 28 threads / cm, 27 threads / cm, the seam head, the stitch density is 35cm / needle, and the thread length at both ends of the seam head is 4cm; the pretreatment liquid includes sodium hypochlorite 12g / L, polyoxygen Ethylene alkylphenol ether 2g / L, potassium permanganate 0.2g / L after padding, the liquid carrying rate is 80%, and then stacked at a constant temperature of 90°C for 45min, and then use polyoxyethylene ether fatty alcohol ether 2g / L and oxalic acid Wash thoroughly with 1g / L hot solution for 5 minutes, then wash twice with cold water. Firstly, 2wt% vat dyes are made into slurry with Swire oil, and then diluted with water according to the fabric to bath ratio of 1:10, then add thiourea dioxide 3g / L, isotridecyl alcohol polyoxyethylene ether 2g / L, glucose 1g / L, sodium silicate 2g / L, sodium sulfide 1g / L, heat up to 45°C at a rate of 1°C / min while stirring, and fully reduce the dye for 20min to obtain the leuc...
Embodiment 2
[0028] Select pure cotton fabric, the warp and weft density is 28 threads / cm, 27 threads / cm, the seam head, the stitch density is 35cm / needle, and the thread length at both ends of the seam head is 3cm; the pretreatment liquid includes sodium hypochlorite 12g / L, polyoxygen Ethylene alkylphenol ether 2g / L, potassium permanganate 0.2g / L after padding, the liquid carrying rate is 80%, and then stacked at a constant temperature of 90°C for 45min, and then use polyoxyethylene ether fatty alcohol ether 2g / L and oxalic acid Wash thoroughly with 1g / L hot solution for 5 minutes, then wash twice with cold water. Then add swire oil dropwise to 2wt% reduced indigo to make a slurry, then dilute with water, then add 3wt% sodium bicarbonate, 6wt% thiourea dioxide, and 6g / L caustic soda, stir and heat up to 45°C to make the dye fully After reducing for 20 minutes, the leuco solution of the vat dye can be obtained; soak the pure cotton fabric, then place it in the leuco solution of the vat dye...
Embodiment 3
[0031] See Table 1 for effect comparison
[0032] Table 1
[0033]
K / S value Example 1 12.17 Example 2 4.52 Example 3 5.23
[0034] Among them, compared with the traditional compounding process of sodium hydrosulfite and thiourea dioxide, the deepening ratio of K / S value after dyeing of the present invention is (12.17-4.52) / 4.52=169%.
[0035] Compared with the traditional compounding process of sodium sulfide and thiourea dioxide, the deepening ratio of K / S value after dyeing of the present invention is (12.17-5.23) / 5.23=133%.
[0036] It can be seen that the dyeing effect of vat dyes can be significantly improved by adopting the dyeing method of the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com