Finishing process for cotton and linen fabric
A fabric, cotton and linen technology, applied in the field of cotton and linen fabric finishing technology, can solve the problem of not feeling soft enough, and achieve the effect of excellent antibacterial, strong washing resistance and soft hand feeling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A finishing process for cotton and linen fabrics, comprising the steps of:
[0021] 1) Put 1-2 parts by weight of sodium alkylarylsulfonate, 0.9 parts by weight of vermiculite powder, 2.2 parts by weight of simethicone, and 1.3 parts by weight of prochloraz into 20 parts by weight of deionized water in sequence, and stir evenly;
[0022] 2) Add 0.9 parts by weight of fluorophenoxyphenylsilane, 1.2 parts by weight of diammonium hydrogen phosphate, 0.2 parts by weight of acetylene carbon black, and 1.7 parts by weight of bis(tallowamidoethyl)-2-hydroxyethylamine , and continue to stir until fully mixed evenly to obtain a finishing solution;
[0023] 3) Pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
Embodiment 2
[0025] The finishing process of cotton and linen fabrics comprises the following steps:
[0026] 1) Put 1 part by weight of sodium alkylarylsulfonate, 0.9 parts by weight of vermiculite powder, 2.2 parts by weight of simethicone, and 1.3 parts by weight of prochloraz into 20 parts by weight of deionized water in sequence, and stir evenly;
[0027] 2) Add 0.9 parts by weight of fluorophenoxyphenylsilane, 1.2 parts by weight of diammonium hydrogen phosphate, 0.2 parts by weight of acetylene carbon black, and 1.7 parts by weight of bis(tallowamidoethyl)-2-hydroxyethylamine , and continue to stir until fully mixed evenly to obtain a finishing solution;
[0028] 3) Pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
Embodiment 3
[0030] The finishing process of cotton and linen fabrics comprises the following steps:
[0031] 1) Put 2 parts by weight of sodium alkylarylsulfonate, 0.9 parts by weight of vermiculite powder, 2.2 parts by weight of simethicone, and 1.3 parts by weight of prochloraz into 20 parts by weight of deionized water in sequence, and stir evenly;
[0032] 2) Add 0.9 parts by weight of fluorophenoxyphenylsilane, 1.2 parts by weight of diammonium hydrogen phosphate, 0.2 parts by weight of acetylene carbon black, and 1.7 parts by weight of bis(tallowamidoethyl)-2-hydroxyethylamine , and continue to stir until fully mixed evenly to obtain a finishing solution;
[0033] 3) Pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology