A wood-plastic composite material and fiber-based technology, which is applied in the field of fiber-based wood-plastic composite materials, can solve the problems of small space for users to choose, single variety of plastic-wood materials, and unsatisfactory performance, and achieve no cracking deformation and good strength. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A fiber-based wood-plastic composite material, including the following components by weight: 40 kg of pineapple leaf fiber base, 35 kg of basalt fiber, 5 kg of polyethylene, 3.5 kg of methylisothiazolinone, 2 kg of benzoin, and methyl phenyl Polyborosiloxane 4kg, polysebacic anhydride 2kg, asbestos 5.5kg, hexamethoxymethyl melamine resin 5kg, camphor wood powder 8kg, ginkgo leaf 6kg, arboria chinensis powder 6kg, agarwood powder 0.1kg, 3-hydroxybenzoic acid 4kg, lauryl sulfate 1kg, plant saponin 4kg, polyamide wax micropowder 0.1kg, white latex 1kg.
[0017] Its preparation method comprises the following steps:
[0018] (1) Add 40kg of pineapple leaf fiber base, 35kg of basalt fiber, 5kg of polyethylene, 3.5kg of methylisothiazolinone, 2kg of benzoin, 4kg of methylphenyl polyborosiloxane, and polydecyl Acid anhydride 2kg, asbestos 5.5kg, hexamethoxymethylmelamine resin 5kg, camphor wood powder 8kg, ginkgo biloba leaf 6kg, arboria chinensis powder 6kg, agarwood powder 0...
Embodiment 2
[0022] A fiber-based wood-plastic composite material, including the following components by weight: 65 kg of pineapple leaf fiber base, 45 kg of basalt fiber, 8 kg of polyethylene, 4.5 kg of methylisothiazolinone, 3 kg of benzoin, and methyl phenyl Polyborosiloxane 6kg, polysebacic anhydride 2.5kg, asbestos 7.5kg, hexamethoxymethyl melamine resin 7kg, camphor wood powder 10kg, ginkgo leaf 8kg, alder wood powder 8kg, agarwood powder 0.2kg, 3-hydroxybenzoic acid 6kg, lauryl sulfate 2kg, plant saponin 6kg, polyamide wax micropowder 0.2kg, white latex 3kg.
[0023] Its preparation method comprises the following steps:
[0024] (1) Add 65kg of pineapple leaf fiber base, 45kg of basalt fiber, 8kg of polyethylene, 4.5kg of methylisothiazolinone, 3kg of benzoin, 6kg of methylphenyl polyborosiloxane, and polydecyl 2.5kg of acid anhydride, 7.5kg of asbestos, 7kg of hexamethoxymethylmelamine resin, 10kg of camphor wood powder, 8kg of ginkgo biloba leaf, 8kg of arboria chinensis powder, ...
Embodiment 3
[0028] A fiber-based wood-plastic composite material, including the following components by weight: 50 kg of pineapple leaf fiber base, 40 kg of basalt fiber, 6 kg of polyethylene, 4 kg of methylisothiazolinone, 3 kg of benzoin, and methyl phenyl Polyborosiloxane 5kg, polysebacic anhydride 2kg, asbestos 6kg, hexamethoxymethyl melamine resin 6kg, camphor wood powder 9kg, ginkgo leaf 6kg, arboria chinensis powder 6kg, agarwood powder 0.1kg, 3-hydroxybenzoic acid 6kg, lauryl sulfate 1kg, plant saponin 6kg, polyamide wax micropowder 0.2kg, white latex 1kg.
[0029] Its preparation method comprises the following steps:
[0030] (1) Add 50kg of pineapple leaf fiber base, 40kg of basalt fiber, 6kg of polyethylene, 4kg of methylisothiazolinone, 3kg of benzoin, 5kg of methylphenyl polyborosiloxane, and polydecyl 2kg of acid anhydride, 6kg of asbestos, 6kg of hexamethoxymethylmelamine resin, 9kg of camphor wood powder, 6kg of ginkgo leaf, 6kg of arboria chinensis powder, 0.1kg of agarw...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com