Briquette binder and use method thereof
A technology of binder and briquette, which is applied in fuel additives, petroleum industry, solid fuel, etc., can solve the problems of many harmful substances, large influence of briquette calorific value, and large sulfur emission, so as to reduce air pollution and make it easy to obtain , the effect of low production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A kind of briquette binding agent, it is made up of guar gum, sucrose, magnesia, wherein sucrose needs through pulverizing, crosses 60 mesh sieves, guar gum, sucrose, magnesia mass ratio is 1:1:1, three Mixed evenly can be used as a binder. When using, take 1kg of coal powder with a particle size of less than 3mm, add 50g of binder, stir and mix evenly, add 200g of water, stir evenly, put it in the mold, add 30MPa pressure for 10-20s, and dry the pressed coal naturally. be usable.
Embodiment 2
[0025] A briquette binder, which consists of fenugreek gum, sucrose, and magnesium oxide, wherein the sucrose needs to be pulverized and passed through a 60-mesh sieve, and the mass ratio of guar gum, sucrose, and magnesium oxide is 2:1:1, and three Those mixed evenly can be used as a binder. When using, take 1kg of coal powder with a particle size of less than 3mm, add 40g of binder, stir and mix evenly, add 200g of water, stir evenly, put it in the mold, add 30MPa pressure for 10-20s, and dry the compressed coal naturally. be usable. When the briquette of this embodiment is burned, it can produce a faint medicinal fragrance.
Embodiment 3
[0027] A briquette binder, which consists of xanthan gum, sucrose, and magnesium oxide, wherein the sucrose needs to be pulverized and passed through a 60-mesh sieve, and the mass ratio of guar gum, sucrose, and magnesium oxide is 2:1:1, and the three Mixed evenly can be used as a binder. When using, take 1kg of coal powder with a particle size of less than 3mm, add 30g of binder, stir and mix evenly, add 200g of water, stir evenly, put it in the mold, add 20MPa pressure for 10-20s, and dry the compressed coal naturally. be usable.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com