Environment-friendly brick and preparation method thereof
A kind of brick and environmental protection technology, applied in the direction of building components, buildings, building structures, etc., can solve the problems of insufficient strength, limited resources, etc., and achieve the effect of simple preparation process, broad market prospect, and good comprehensive performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] An environmentally friendly brick, which is composed of the following raw materials in parts by weight: 15 parts of coal ash, 0.5 part of brown sugar, 1 part of glutinous rice flour, 25 parts of steel slag, 10 parts of marble waste pulp, 2 parts of resin, 1 part of polyethylene glycol, natural 8 parts of fiber material and 0.2 part of vitrified microspheres. The resin is silicone resin and the natural fiber materials include a blend of rice husk, coconut shell and bamboo.
[0019] The preparation method of described environmental protection brick, concrete steps are as follows:
[0020] Step 1, soaking the mixture of rice husk, coconut shell and bamboo with water and pulverizing, mixing the pulverized rice husk, coconut shell and bamboo mixture, marble waste slurry and clear water in a container, sealing, soaking and fermenting, and then Add brown sugar and stir, seal up and complete, and obtain the first mixture;
[0021] Step 2, putting steel slag, silicone resin an...
Embodiment 2
[0026] An environmentally friendly brick is composed of the following raw materials in parts by weight: 17 parts of coal ash, 0.8 parts of brown sugar, 1.5 parts of glutinous rice flour, 32 parts of steel slag, 16 parts of marble waste pulp, 3 parts of resin, 2 parts of polyethylene glycol, natural 11 parts of fiber material and 0.4 parts of vitrified microspheres. The vitrified microbeads are hydrophobic vitrified microbeads, and the particle size of the vitrified microbeads is 12um.
[0027] The preparation method of described environmental protection brick, concrete steps are as follows:
[0028] Step 1: Wet the natural fiber material with water and pulverize it, mix the pulverized natural fiber material, marble waste slurry and clear water in a container, seal, soak and ferment, then add brown sugar for stirring, and seal up to obtain the first mixture ;
[0029] Step 2, putting steel slag, resin and hydrophobic vitrified microspheres into a ball mill and adding ball mil...
Embodiment 3
[0034] An environmentally friendly brick, which is composed of the following raw materials in parts by weight: 21 parts of coal ash, 1.2 parts of brown sugar, 2.5 parts of glutinous rice flour, 38 parts of steel slag, 22 parts of marble waste slurry, 4 parts of resin, 3 parts of polyethylene glycol, natural 13 parts of fiber material and 0.6 parts of vitrified microspheres. The resin is silicone resin and the natural fiber materials include a blend of coconut husk, wheat husk and bagasse.
[0035] The preparation method of described environmental protection brick, concrete steps are as follows:
[0036] Step 1: Soak the mixture of coconut husk, wheat husk and bagasse in water and crush it, mix the crushed coconut husk, wheat husk and bagasse, marble waste pulp and water in a container, seal, soak and ferment , and then add brown sugar for stirring, and the storage is completed to obtain the first mixture;
[0037] Step 2, putting steel slag, silicone resin and vitrified micr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com