Unlock instant, AI-driven research and patent intelligence for your innovation.

Pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent as well as preparation method and application thereof

A technology of fluorescent whitening agent and tetradecyl, which is applied in the field of fluorescent whitening agent, can solve the problem of lack of fluorescent whitening agent of heavy calcium carbonate powder, etc., achieve strong ultraviolet absorption performance, simple synthesis method, combined The effect of high firmness

Active Publication Date: 2017-12-08
HEZHOU UNIV
View PDF2 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] The surface of heavy calcium carbonate powder has free calcium ions and hydroxyl groups. It is difficult for the existing fluorescent whitening agents on the market to ionically bond or adsorb on the surface of heavy calcium carbonate powder, so they lack the ability to effectively whiten and brighten heavy calcium carbonate powder Fluorescent whitening agent for calcium carbonate powder

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent as well as preparation method and application thereof
  • Pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent as well as preparation method and application thereof
  • Pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent as well as preparation method and application thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0028] Add 21mmol of 2,4-dichloropyrimidine to 22mL of dimethylformamide and stir at 25°C. Then dropwise add a mixture of 10mmol 4,4'-diaminostilbene-2,2'-disulfonic acid and 100mL distilled water, and use 10%Na 2 CO 3 The pH of the reaction system was maintained at 7 by the aqueous solution, and the reaction was carried out at 25° C. for 11 h. Then add 19.5mmol dimethyltetradecylamine, with 10% Na 2 CO 3 The aqueous solution maintained the pH of the system at 9, and the reaction was refluxed for 7 hours. The end point of the two-step reaction was monitored by thin-layer chromatography. Cool to room temperature, add 20 g of sodium chloride, stir, filter with suction, and dry in vacuum to obtain pyrimidine-tetradecyl quaternary ammonium salt fluorescent whitening agent with a yield of 87%.

Embodiment 2

[0030] Add 21mmol 2,4-dichloropyrimidine to 31.5mL dimethylformamide and stir at 20°C. Then dropwise add a mixture of 10mmol 4,4'-diaminostilbene-2,2'-disulfonic acid and 110mL distilled water, with 10%Na 2 CO 3 The pH of the reaction system was maintained at 8 with the aqueous solution, and the reaction was carried out at 25° C. for 10 h. Then add 19.5mmol dimethyltetradecylamine, with 10% Na 2 CO 3 The pH of the system was maintained at 8 with the aqueous solution, and the reaction was refluxed for 6 hours. The end point of the two-step reaction was monitored by thin-layer chromatography. Cool to room temperature, add 20 g of sodium chloride, stir, filter with suction, and dry in vacuum to obtain pyrimidine-tetradecyl quaternary ammonium salt fluorescent whitening agent with a yield of 83%.

Embodiment 3

[0032] Add 21mmol 2,4-dichloropyrimidine to 26mL dimethylformamide and stir at 25°C. Then dropwise add a mixture of 10mmol 4,4'-diaminostilbene-2,2'-disulfonic acid and 100mL distilled water, and use 10%Na 2 CO 3 The pH of the reaction system was maintained at 7.5 with the aqueous solution, and the reaction was carried out at 25°C for 11 hours. Then add 19.5mmol dimethyltetradecylamine, with 10% Na 2 CO 3 The aqueous solution maintained the pH of the system at 9, and the reaction was refluxed for 7 hours. The end point of the two-step reaction was monitored by thin-layer chromatography. Cool to room temperature, add 20 g of sodium chloride, stir, filter with suction, and dry in vacuum to obtain pyrimidine-tetradecyl quaternary ammonium salt fluorescent whitening agent with a yield of 84.5%.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
whitenessaaaaaaaaaa
Login to View More

Abstract

The invention provides a pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent, which is characterized in that a structural formula of the pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent is as shown in the description. The invention aims to provide the pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent as well as a preparation method and application thereof. The preparation method is simple, and the raw materials are cheap. Heavy calcium carbonate powder treated by adopting the pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent provided by the invention has higher whiteness and brightness, and the pyrimidine-myristyl quaternary ammonium salt fluorescent whitening agent is the high-performance heavy calcium carbonate powder fluorescent whitening agent.

Description

technical field [0001] The invention relates to the technical field of fluorescent whitening agents, in particular to a pyrimidine-tetradecyl quaternary ammonium fluorescent whitening agent and a preparation method and application thereof. Background technique [0002] In my country's "12th Five-Year" new material development plan, the development of new materials that are coordinated with resources and the environment is taken as the main assessment index, and the problem of resource shortage is solved through the development of new materials. my country has formed a relatively complete material science and technology system, and has obvious resource advantages and technological advantages in some new material fields, but the overall independent innovation capability is still relatively weak, and there are still relatively few new material products and technologies with independent intellectual property rights. Especially in terms of ground calcium carbonate powder fluoresce...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C07D239/22C09B57/00C09K11/06C09C1/02C09C3/08
CPCC01P2004/61C01P2006/60C07D239/22C09B57/00C09C1/021C09C3/08C09K11/06C09K2211/1007C09K2211/1044
Inventor 万茂生画莉
Owner HEZHOU UNIV