Preparation technology and application of modified film fabric
A preparation process and membrane cloth technology, which is applied to the preparation process of modified membrane cloth and its application field, can solve the problems of increasing the manufacturing cost of modified membrane cloth, inability to add volatile components to the modified membrane cloth, and shorten the rehydration time. effect of time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0067] In the preparation process provided by the invention, the volatile components and / or heat-sensitive components are coated on the membrane cloth in the form of anhydrous coating liquid, without subsequent dehydration. Since dehydration is not required, the volatilization of volatile components during dehydration of the membrane cloth is avoided, so this process solves the problem that volatile substances cannot be added to the modified membrane cloth. At the same time, since dehydration is not required, heat-sensitive components can also be added to the modified membrane cloth without using a freeze-drying process. In addition, the preparation process provided by the present invention enables the thickener to be coated on the membrane cloth without being mixed with water or grease, which can shorten the rehydration time of the modified membrane cloth when rehydration is used.
[0068] In addition, the preparation process of the modified membrane cloth provided by the pre...
Embodiment 1
[0073] The modified xanthan gum (Nissin, model Nomcort ZZ) is stirred and dissolved with water to make a high molecular polymer aqueous solution with a content of 0.2wt%, and the non-woven medicinal application is immersed in the above aqueous solution, and then the above film cloth Put it into a hot air circulation oven to remove moisture to obtain a pre-coated polymer patch, and the ratio of modified xanthan gum to the patch is 1g / m 2 ;Menthol at 0.1g / m 2 Spray directly onto the dehydrated patch; pack the salicylate and the above-mentioned patch separately to obtain a new type of medicinal patch combination product.
[0074] After the above-mentioned new patch is packaged, the number of microorganisms in the package can be kept within 36 months to meet the cosmetic specification range (2 The proportion of the pre-coated polymer patch is added to form a new type of analgesic patch with a mint aroma; the above-mentioned analgesic patch is placed on the skin surface, and the fi...
Embodiment 2
[0079] Disperse hydrogenated polydecene (Nissin, model HP-30) and polyacrylamide according to the mass ratio of 5:1 to obtain a dispersion; 2 The ratio of 1,2-propanediol and lavender essential oil is mixed with each other according to the mass ratio of 5:1, and 0.5g / m 2 Spray evenly on the surface of the patch; pack separately with biological factors such as EGF and bFGF extracted from milk, and sterile saline to obtain a new type of medicinal patch combination package.
[0080] After the above-mentioned new mask is packaged, the number of microorganisms in the package can be kept within 36 months within the cosmetic specification range (2 The ratio of sterile physiological saline to dissolve biological factors to form a solution, the solution is added to the pre-coated polymer patch to form a new type of drug patch; the drug patch on the skin surface, keep the membrane cloth in a vertical state, can maintain More than 30 minutes, and the membrane cloth is still moist and clo...
PUM
Property | Measurement | Unit |
---|---|---|
coating mass | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com