Textile raw material staining method with stable staining

A dyeing method and technology of raw materials, applied in the field of printing and dyeing, can solve the problems affecting the fullness and color fastness of finished fabrics, and the effect of fabric printing and dyeing is not ideal, so as to improve the fullness and color fastness, improve the color fastness, and stabilize the color and luster. Effect

Inactive Publication Date: 2018-03-20
HUZHOU NANXUN JINJIBAO TEXTILE
View PDF3 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, when dealing with the dyeing of such fabrics, the printing and dyeing effect of the fabric is not ideal due to the limitation of the process, which affects the fullness and color fastness of the finished fabric.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] Example 1. A method for dyeing textile raw materials with stable dyeing, comprising the steps of:

[0018] Step 1: Add dyeing agent and water into the dyeing vat, stir evenly, raise the temperature to 55°C at a heating rate of 3°C, keep it for 1.5h, add carbonic acid to adjust the pH of the dyeing solution to 5;

[0019] Step 2: Soak the textile raw material in the dyeing vat for 1.5 hours, then raise the temperature at a rate of 2°C / min to 93°C and keep it for 2.5h; the bath ratio of the textile raw material is 1:18;

[0020] Step 3: drying, drying the soaked textile raw materials at 85°C;

[0021] Step 4: Rinse, take out the dried textile raw material and soak it in clean water for 35 minutes, and add rinse agent;

[0022] Step 5: dry, take out the rinsed textile raw materials and dry naturally; the dyeing agent is made of the following raw materials in parts by weight: 8 parts of diphenyl ether tetra-acid dianhydride, 5 parts of polypropylene glycol, 18 parts of mi...

Embodiment 2

[0023] Example 2. A method for dyeing textile raw materials with stable dyeing, comprising the steps of:

[0024] Step 1: Add dyeing agent and water into the dyeing vat, stir evenly, raise the temperature to 60°C at a heating rate of 4°C, keep it for 1.5h, add carbonic acid to adjust the pH of the dyeing solution to 5;

[0025] Step 2: Soak the textile raw material in the dyeing vat for 3.5 hours, then raise the temperature at a rate of 3°C / min to 96°C and keep it for 2.5h; the liquor ratio of the textile raw material is 1:18;

[0026] Step 3: drying, drying the soaked textile raw materials at 90°C;

[0027] Step 4: Rinse, take out the dried textile raw material and soak it in clean water for 55 minutes, and add rinse agent;

[0028] Step 5: dry, take out the rinsed textile raw materials and dry naturally; the dyeing agent is made of the following raw materials in parts by weight: 10 parts of diphenyl ether tetra-acid dianhydride, 2 parts of polypropylene glycol, 20 parts of...

Embodiment 3

[0029] Example 3. A method for dyeing textile raw materials with stable dyeing, comprising the steps of:

[0030] Step 1: Add dyeing agent and water into the dyeing vat, stir evenly, raise the temperature to 57°C at a heating rate of 3.5°C, keep it for 1.5h, add carbonic acid to adjust the pH of the dyeing solution to 5;

[0031] Step 2: Soak the textile raw material in the dyeing vat for 2.5 hours, then raise the temperature at a rate of 2.5°C / min, raise the temperature to 95°C and keep it for 2.5h; the bath ratio of the textile raw material is 1:18;

[0032] Step 3: drying, drying the soaked textile raw materials at 87°C;

[0033] Step 4: Rinse, take out the dried textile raw material and soak it in clean water for 45 minutes, and add rinse agent;

[0034] Step 5: dry, take out the rinsed textile raw materials and dry naturally;

[0035] The dyeing agent is made of the following raw materials in parts by weight: 9 parts of diphenyl ether tetra-acid dianhydride, 4 parts of...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a textile raw material staining method with stable staining. The textile raw material staining method comprises the following steps: S1: in a staining jar, adding stain and water, evenly stirring, raising temperature to 55-60 DEG C through a 3-4 DEG C temperature raising rate, keeping for 1.5h, and adding carbonic acid to regulate the pH (Potential of Hydrogen) of stainingliquid to 5; S2: dipping texture raw materials in the staining jar for 1.5-3.5h, then, raising the temperature at the speed of 2-3 DEG C / min, raising the temperature to 93-96 DEG C, and keeping for 2.5h, wherein the bath ratio of the texture raw material is 1:18; S3: drying; S4: rinsing; S5: drying. The stain is prepared from the following raw materials in parts by weight: 8-10 parts of 4-[(1,3-Dihydro-1,3-dioxo-5-isobenzofuranyl)oxy]-1,3-isobenzofurandione, 2-5 parts of polypropylene glycol, 18-20 parts of mica powder, 2-5 parts of zinc stearate, 4-7 parts of propyl acetate, 9-12 parts of iron oxide red, 7-10 parts of ethyl triethoxysilane, 6-12 parts of sodium hydroxide, 4-7 parts of sodium carbonate, 3-5 parts of ethyl alcohol, 40-45 parts of water and 5-8 parts of polyvinylpyrrolidone.

Description

technical field [0001] The invention relates to the field of printing and dyeing, in particular to a method for dyeing textile raw materials with stable dyeing. Background technique [0002] With the improvement of people's living standards, people's requirements for textiles are getting higher and higher. A large number of fabrics blended by fibers of different properties have emerged on the market, so that the fabrics have the characteristics of different fibers simultaneously. Commonly used are polyester-cotton blended fabrics, which are woven by blending polyester and cotton. On the one hand, polyester fibers have the characteristics of high strength and good wrinkle resistance, and at the same time, cotton has the advantages of good hygroscopicity and comfortable wearing. However, when dealing with the dyeing of this type of fabric, the printing and dyeing effect of the fabric is not ideal due to the limitation of the process, which affects the fullness and color fastn...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): D06P1/673D06P1/52D06P1/651D06P1/613D06P1/653
CPCD06P1/673D06P1/5242D06P1/6138D06P1/65106D06P1/65125D06P1/65143D06P1/6533D06P1/6735D06P1/67383D06P5/002
Inventor 方国健潘伟丽
Owner HUZHOU NANXUN JINJIBAO TEXTILE