[0025] A pavement moisture permeameter, which includes a metal shell, the metal shell has been treated with film coating, and the film coating process includes the following steps:
[0026] 1) Put 2 to 3 parts by weight of acrylic resin, 3.0 parts by weight of brominated diethyl carbonate, 1.5 parts by weight of polymerized linseed oil, and 0.7 parts by weight of high-chlorinated polyethylene resin into 50 parts by weight of deionized water in sequence, Stir well;
[0027] 2) Add 11.0 parts by weight of vinyl ethyl carbonate, 8.0 parts by weight of hydroxypropyl methylcellulose, 1.8 parts by weight of vanadium isooctanoate, and 1.2 parts by weight of borosilicate glass frit in turn, and continue stirring until fully mixed, Prepare the coating treatment liquid;
[0028] 3) Put the metal shell into the coating treatment solution for immersion, take it out and dry it.
Embodiment 2
[0030] A pavement moisture permeameter, which includes a metal shell, the metal shell has been treated with film coating, and the film coating process includes the following steps:
[0031] 1) Put 2 parts by weight of acrylic acid resin, 3.0 parts by weight of brominated diethyl carbonate, 1.5 parts by weight of polymerized linseed oil, and 0.7 parts by weight of high-chlorinated polyethylene resin into 50 parts by weight of deionized water in sequence, and stir evenly ;
[0032] 2) Add 11.0 parts by weight of vinyl ethyl carbonate, 8.0 parts by weight of hydroxypropyl methylcellulose, 1.8 parts by weight of vanadium isooctanoate, and 1.2 parts by weight of borosilicate glass frit in turn, and continue stirring until fully mixed, Prepare the coating treatment liquid;
[0033] 3) Put the metal shell into the coating treatment solution for immersion, take it out and dry it.
Embodiment 3
[0035] A pavement moisture permeameter, which includes a metal shell, the metal shell has been treated with film coating, and the film coating process includes the following steps:
[0036] 1) Put 3 parts by weight of acrylic acid resin, 3.0 parts by weight of brominated diethyl carbonate, 1.5 parts by weight of polymerized linseed oil, and 0.7 parts by weight of high-chlorinated polyethylene resin into 50 parts by weight of deionized water in sequence, and stir evenly ;
[0037] 2) Add 11.0 parts by weight of vinyl ethyl carbonate, 8.0 parts by weight of hydroxypropyl methylcellulose, 1.8 parts by weight of vanadium isooctanoate, and 1.2 parts by weight of borosilicate glass frit in turn, and continue stirring until fully mixed, Prepare the coating treatment liquid;
[0038] 3) Put the metal shell into the coating treatment solution for immersion, take it out and dry it.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com