A kind of environment-friendly concrete curing agent and preparation method thereof
An environment-friendly concrete and curing agent technology, applied in the field of building materials, can solve problems such as difficult construction, unsatisfactory curing effect, laborious and laborious, etc., and achieve the effect of convenient operation, large-scale industrial production, and simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0072] In another embodiment, the present application also provides the preparation method of the environment-friendly concrete curing agent, which includes the following steps: under stirring conditions, adding hydrogen peroxide to the mixture A, then dropwise adding solution B, solution C, Solution D, carry out a polymerization reaction, adjust the viscosity of the reaction solution with xanthan gum, and then adjust it with water to a solid content of 15wt%, which is an environmentally friendly concrete curing agent;
[0073] The mixture A is obtained by mixing vinyl glycol polyoxyethylene ether, sulfonated graphene and water;
[0074] The solution B is obtained by mixing acrylic acid, hydroxyethyl acrylate, mercaptoethanol and water;
[0075] The solution C is obtained by mixing the reducing agent TP1351 and water;
[0076] The solution D is obtained by mixing styrene and water.
[0077] Preferably, the preparation method of the environment-friendly concrete curing agent ...
Embodiment 1
[0095] (1) Preparation before polymerization:
[0096] Preparation of mixture A: Weigh 100 parts by weight of vinyl glycol polyoxyethylene ether with a number average molecular weight of 1200, 5 parts of sulfonated graphene and 500 parts by weight of water, put them into a polymerization reactor, stir evenly, and heat up to 10℃, standby;
[0097] Preparation of Solution B: Weigh 50 parts by weight of acrylic acid, 20 parts by weight of hydroxyethyl acrylate, 4 parts by weight of mercaptoethanol and 100 parts by weight of water, stir evenly, and prepare dropwise;
[0098] Preparation of solution C: weigh 1 part by weight of reducing agent TP1351 and 200 parts by weight of water, stir evenly, and prepare dropwise;
[0099] Preparation of solution D: weigh 50 parts by weight of styrene and 100 parts by weight of water, stir evenly, and prepare to add dropwise;
[0100] (2) Polymerization: In step (1), the polymerization reactor that has been put into the mixture A is started to...