A technology for safety airbags and ignition powders, which is applied to the generation of compressed gas, explosives, and offensive equipment. It can solve the problems of poor thermal stability, high risk factor for automatic ignition powders, and poor long-term storage stability. Good heat storage stability and high temperature long-term storage stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0024] The present invention also provides the preparation method of the automatic ignition powder, which comprises mixing fuel, oxidant, auxiliary oxidant and additive to obtain a mixture, and then granulating, drying and pressing the mixture to obtain the automatic ignition powder.
[0025] As mentioned above, the autoignition powder may also contain various binders commonly used in the prior art, therefore, the preparation method also includes the step of adding binders to the mixture. Preferably, in order to facilitate the uniform mixing of the binder and other components in the medicament, the binder is preferably added in the form of a solution, for example, the binder may be dissolved in a solvent first, and then added to the mixture. Preferably, based on 100 parts by weight of the binder solution, the amount of solvent used is 98 parts by weight. The solvent may be various organic solvents common in the prior art, such as at least one selected from acetone, ethanol, an...
preparation example 1
[0030] Add 3 parts by weight of bamboo charcoal material into a solution containing 3 parts by weight of copper phthalocyanine, stir and impregnate for 24 hours, filter, wash, and dry at 100°C for 8 hours to obtain metal phthalocyanine / bamboo charcoal material A1 with a particle size of 75-150 µm. The load of metal phthalocyanine in the metal phthalocyanine / bamboo charcoal material is 40% (weight).
preparation example 2
[0032] Add 4 parts by weight of bamboo charcoal material to a solution containing 1 part by weight of iron phthalocyanine, stir and impregnate for 24 hours, filter, wash, and dry at 100°C for 8 hours to obtain metal phthalocyanine / bamboo charcoal material A2 with a particle size of 75-150 µm. The load of metal phthalocyanine in the metal phthalocyanine / bamboo charcoal material is 20% (weight).
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
The average particle size | aaaaa | aaaaa |
The average particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com