[0030] The specific preparation method of the friction material for the piezoelectric motor may include the following steps:
[0031] (1) Mix the raw materials according to the formula quantity, dry the mixed mixture, and pulverize it; preferably use the wet mixing method, that is, mix the raw materials with absolute ethanol;
[0032] (2) Pour the mixed material processed in step (1) into a mold, cold press it at a pressure of 38-43 MPa, and demould, to obtain a friction material preform;
[0033] (3) Sintering the preform in a high-temperature sintering furnace at 330-350° C. to obtain the friction material.
Embodiment 1
[0037] This embodiment provides a friction material for a piezoelectric motor. In terms of weight percentage, the raw materials of the friction material include: 40wt% polytetrafluoroethylene, 15wt% polyetheretherketone, 5wt% polyphenylene, carbon fiber 20wt%, glass fiber 5wt%, aluminum oxide 5wt%, molybdenum disulfide 10wt%;
[0038] Concrete preparation steps are:
[0039] a) Weigh each raw material according to the formula quantity, add an appropriate amount of absolute ethanol, and mix at high speed with a planetary ball mill to make each component mix evenly;
[0040] b) Dry the mixture in step a) at 100°C for 4 hours, crush it, and sieve it through a 200-mesh sieve;
[0041]c) Pour the mixed material processed in step b) into a mold for cold press molding, the molding pressure is 40Mpa, and the mold is demoulded after holding the pressure for 15 minutes to obtain a friction material preform;
[0042] d) putting the friction material pre-product into a high-temperature ...
Embodiment 2
[0046] This embodiment provides a friction material for a piezoelectric motor. In terms of weight percentage, the raw materials of the friction material include: 45wt% polytetrafluoroethylene, 10wt% polyetheretherketone, 5wt% polyphenylene, carbon fiber 15wt%, glass fiber 10wt%, aluminum oxide 5wt%, molybdenum disulfide 10wt%;
[0047] Concrete preparation steps are:
[0048] a) Weigh each raw material according to the formula quantity, add an appropriate amount of absolute ethanol, and mix at high speed with a planetary ball mill to make each component mix evenly;
[0049] b) Dry the mixture in step a) at 100°C for 4 hours, crush it, and sieve it through a 200-mesh sieve;
[0050] c) Pour the mixed material processed in step b) into a mold for cold press molding, the molding pressure is 40Mpa, and the mold is demoulded after holding the pressure for 15 minutes to obtain a friction material preform;
[0051] d) putting the friction material pre-product into a high-temperatur...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com