Preparation method of low-cost polycarboxylate water reducer
A technology of polycarboxylic acid and water reducing agent, which is applied in the field of concrete admixture and building materials, can solve the problems of complex performance degradation process of water reducing agent, unfavorable large-scale production, complicated production steps, etc., to avoid rapid reduction of reactivity, The preparation process and required equipment are simple and the effect of strong reactivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] A kind of preparation method of low-cost polycarboxylate water reducer, it is characterized in that, comprises the following steps:
[0031] 1) Add 270 parts of allyl polyoxyethylene ether, 75 parts of Kewei chemical industrial grade carboxymethyl starch, 15 parts of acrylic acid and 300 parts of water into the reaction kettle, stir to dissolve;
[0032] 2) Measure the temperature in the kettle, control the temperature at 55°C, and after the temperature is stable, add 1.5 parts of hydrogen peroxide at one time;
[0033]3) After adding hydrogen peroxide for 5 minutes, start to drop the initiator and the small monomer solution in sequence. After the initiator is added, start to add the small monomer solution dropwise within 10 minutes. The small monomer solution dripping time is 5.5 hours, and the initiator dropping time It was 6 hours; the initiator was made up of 1.5 parts of thioglycolic acid, 0.4 parts of vitamin C and 120 parts of water, and the small monomer solutio...
Embodiment 2
[0036] A kind of preparation method of low-cost polycarboxylate water reducer, it is characterized in that, comprises the following steps:
[0037] 1) Add 273 parts of methallyl polyoxyethylene ether, 80 parts of Yanxing chemical industrial grade carboxymethyl starch, 13 parts of acrylic acid and 280 parts of water into the reaction kettle, stir to dissolve;
[0038] 2) Measure the temperature in the kettle and control the temperature at 54°C. After the temperature is stable, add 1.8 parts of hydrogen peroxide at one time;
[0039] 3) After adding hydrogen peroxide for 5 minutes, start to drop the initiator and the small monomer solution in sequence. After the initiator is added, start to add the small monomer solution dropwise within 10 minutes. The small monomer solution is added for 6 hours, and the initiator is added. It was 6.5 hours; the initiator was made up of 1.3 parts of thioglycolic acid, 0.5 parts of vitamin C and 110 parts of water, and the small monomer solution ...
Embodiment 3
[0042] A kind of preparation method of low-cost polycarboxylate water reducer, it is characterized in that, comprises the following steps:
[0043] 1) Add 293 parts of vinyl butyl ether polyoxyethylene ether, 55 parts of Xinglei chemical industrial grade carboxymethyl starch, 11 parts of acrylic acid and 250 parts of water into the reaction kettle, stir to dissolve;
[0044] 2) Measure the temperature in the kettle, control the temperature at 53°C, and after the temperature is stable, add 2.5 parts of hydrogen peroxide at one time;
[0045] 3) After adding hydrogen peroxide for 5 minutes, start to drop the initiator and the small monomer solution in sequence. After the initiator is added, start to add the small monomer solution dropwise within 10 minutes. The small monomer solution is added for 5 hours, and the initiator is added. It was 5.5 hours; the initiator was made up of 1.1 parts of thioglycolic acid, 0.6 parts of vitamin C and 100 parts of water, and the small monomer ...