Non-metal carbon fiber recombination line clutch facing and preparation method thereof
A technology of clutch face plate and composite wire, which is applied in the direction of clutches, friction clutches, mechanically driven clutches, etc., can solve problems affecting the performance of automobiles, poor quality of clutch plates, unstable internal structures, etc., and improve the safety performance and stability of use Excellent performance, high temperature resistance, and the effect of solving aging problems
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A metal-free carbon fiber composite wire clutch face sheet, comprising a composite cloth woven by high-strength composite wires and a coating uniformly impregnated on its surface, the raw materials of the high-strength composite wires are as follows in parts by weight: 55 parts of thermoplastic resin, 3 parts of boron trifluoride monoethylamine, 1 part of antioxidant, 15 parts of carbon fiber, 15 parts of basalt fiber, 15 parts of polyacrylonitrile fiber, 15 parts of high temperature resistant ceramic fiber, 2 parts of AG80 epoxy resin;
[0020] The high-strength composite wire is twisted from basalt fiber wire, polyacrylonitrile fiber wire, high-temperature resistant ceramic fiber wire and carbon fiber wire;
[0021] The raw materials of the coating are as follows in parts by weight: 30 parts of modified phenolic resin; 2 parts of beryllium bronze powder; 15 parts of nano silicon dioxide; 1.0 part of antioxidant; 1 part of magnesium stearate; 1.0 part of tricresyl phosp...
Embodiment 2
[0032] A metal-free carbon fiber composite wire clutch face sheet, including a composite cloth woven by high-strength composite wires and a coating uniformly impregnated on its surface, the raw materials of the high-strength composite wires are as follows in parts by weight: 60 parts of thermoplastic resin, 5 parts of boron trifluoride monoethylamine, 3 parts of antioxidant, 20 parts of carbon fiber, 20 parts of basalt fiber, 20 parts of polyacrylonitrile fiber, 20 parts of high temperature resistant ceramic fiber, 3 parts of AG80 epoxy resin;
[0033] The high-strength composite wire is twisted from basalt fiber wire, polyacrylonitrile fiber wire, high-temperature resistant ceramic fiber wire and carbon fiber wire;
[0034] The raw materials of the coating are as follows in parts by weight: 40 parts of modified phenolic resin; 3 parts of beryllium bronze powder; 25 parts of nano silicon dioxide; 1.6 parts of antioxidant; 2 parts of magnesium stearate; 1.3 parts of tricresyl ph...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com