A technology of kaolin and ore slurry, applied in separation methods, chemical instruments and methods, filtration separation, etc., can solve problems such as difficult dehydration and long dehydration time, and achieve the effects of reduced suspension, increased production capacity, and shortened filter press dehydration time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Embodiment 1: A method for improving the dehydration efficiency of kaolin slurry
[0026] The method in turn includes the following steps:
[0027] The first step is to hydrate the raw kaolin ore into raw pulp, and then classify the raw pulp through a hydrocyclone with a diameter of 75 mm to obtain a pulp. The mass concentration of the pulp is 15%~20%, and the viscosity of the pulp is less than 1000mPa. s, the laser particle size of kaolin in the slurry is 3.5 microns, and the microstructure is tubular;
[0028] The second step is to import the pulp into the pulp tank 1, stir the pulp, and then add calcium oxide to the pulp. The amount of calcium oxide added is 0.05% of the dry ore weight in the pulp. After stirring for 5-10 minutes quickly, the pH value of the pulp will increase. to 7.0~8.0; then, add polyacrylamide with a molecular weight of 12 million to the pulp, the amount of polyacrylamide added is 2 / 100000 of the weight of dry ore in the pulp, stir slowly for 2~...
Embodiment 2
[0035] Embodiment 2: A method for improving the dehydration efficiency of kaolin slurry
[0036] The method in turn includes the following steps:
[0037] The first step is to hydrate the raw kaolin ore into raw pulp, and then classify the raw pulp through a hydrocyclone with a diameter of 55 mm to obtain a pulp. The mass concentration of the pulp is 15%~20%, and the viscosity of the pulp is less than 1000mPa. s, the laser particle size of kaolin in the slurry is 3.0 microns, and the microstructure is segmented;
[0038] The second step is to import the pulp into the pulp tank, stir the pulp, and then add calcium oxide to the pulp. The amount of calcium oxide added is 0.03% of the dry ore weight in the pulp. After stirring for 5-10 minutes quickly, the pH value of the pulp rises to Between 7.0 and 8.0; then, add polyacrylamide with a molecular weight of 12 million to the pulp, the amount of polyacrylamide added is one millionth of the dry ore weight in the pulp, stir slowly f...