Embodiment 1
[0022] A photochromic Jun enamel, which is prepared from the following raw materials in parts by weight: 13-19 parts of feldspar, 25-31 parts of quartz, 9-15 parts of calcite, 2-4 parts of Suzhou soil, and 17-23 parts of this medicine , 13-19 parts of nano-tungsten oxide, 1.5-2.5 parts of nano-titanium oxide, and 0.5-1.5 parts of nano-zinc oxide.
[0023] The preparation method of the above-mentioned photochromic Jun enamel is characterized in that it comprises the following steps:
[0024] (1) Preparation of tungsten oxide-titanium oxide-zinc oxide color-changing powder: Weigh the above-mentioned nano-tungsten oxide, nano-titanium oxide, and nano-zinc oxide, add absolute ethanol and ball mill for 20-40min, dry, at 1300-1320℃ Calcined at low temperature for 30-40 minutes to obtain tungsten oxide-titanium oxide-zinc oxide discoloration powder;
[0025] (2) Preparation of glaze slurry: mix the above-mentioned feldspar, quartz, calcite, Suzhou soil, this medicine with tungsten o...
Embodiment 2
[0039] A photochromic Jun enamel, which is prepared from the following raw materials in parts by weight: 16 parts of feldspar, 28 parts of quartz, 12 parts of calcite, 3 parts of Suzhou soil, 20 parts of this medicine, 16 parts of nano-tungsten oxide, 2 parts of titanium, 1 part of nano zinc oxide.
[0040] The preparation method of the above-mentioned photochromic Jun enamel is characterized in that it comprises the following steps:
[0041] (1) Preparation of tungsten oxide-titanium oxide-zinc oxide color-changing powder: Weigh the above-mentioned nano-tungsten oxide, nano-titanium oxide, and nano-zinc oxide, add absolute ethanol and ball mill for 30 minutes, dry, and calcinate at 1310°C for 35 minutes. Obtain tungsten oxide-titanium oxide-zinc oxide discoloration powder;
[0042] (2) Preparation of glaze slurry: mix the above-mentioned feldspar, quartz, calcite, Suzhou soil, this medicine with tungsten oxide-titanium oxide-zinc oxide discoloration powder, pulverize, ball m...
Embodiment 3
[0053] A photochromic Jun enamel, which is prepared from the following raw materials in parts by weight: 15 parts of feldspar, 27 parts of quartz, 14 parts of calcite, 2 parts of Suzhou soil, 23 parts of this medicine, 15 parts of nano-tungsten oxide, and 15 parts of nano-oxidized tungsten 2.5 parts of titanium, 1.5 parts of nano zinc oxide.
[0054] The preparation method of the above-mentioned photochromic Jun enamel is characterized in that it comprises the following steps:
[0055] (1) Preparation of tungsten oxide-titanium oxide-zinc oxide color-changing powder: Weigh the above-mentioned nano-tungsten oxide, nano-titanium oxide, and nano-zinc oxide, add absolute ethanol and ball mill for 40 minutes, dry, and calcinate at 1320°C for 30 minutes. Obtain tungsten oxide-titanium oxide-zinc oxide discoloration powder
[0056] (2) Preparation of glaze slurry: mix the above-mentioned feldspar, quartz, calcite, Suzhou soil, this medicine with tungsten oxide-titanium oxide-zinc ox...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com