Precipitation reagent for processing leather waste water, and preparation method thereof
A technology of leather wastewater and reagents, applied in the direction of special treatment targets, water/sewage treatment, chemical instruments and methods, etc., can solve the problems of natural pollution, water quality pollution, lack, etc., achieve good deodorization effect, improve water quality, and reduce costs low effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0016] A method for preparing a precipitation reagent for treating leather wastewater, comprising the following steps,
[0017] A. Add calcium carbonate, diatomaceous earth, bentonite, activated carbon particles, nano-zinc oxide, nano-calcium oxide, and nano-alumina to a grinder for grinding, and then pass through a 100-mesh sieve to obtain a mixture A;
[0018] B. Add modified potassium hydroxide to the mixture A, mix and add to the stirring tank for full stirring, the stirring speed is 800 rpm, and the time is 40min, to obtain the mixture B;
[0019] C. Add nano-silver particle powder into mixture B, mix it and put it into a high-speed kneader, heat it to 60°C, and stir for 35 minutes to get it.
Embodiment
[0020] Embodiment: the precipitation reagent of processing leather waste water, is made of the raw material of following parts by weight,
[0021] 22 parts of nano-calcium oxide, 16 parts of modified potassium hydroxide, 13 parts of calcium carbonate, 11 parts of diatomite, 16 parts of bentonite, 17 parts of activated carbon particles, 23 parts of nano-zinc oxide, 23 parts of nano-alumina, and nano-silver particle powder 7 servings.
[0022] A method for preparing a precipitation reagent for treating leather wastewater, comprising the following steps,
[0023] A. Add calcium carbonate, diatomaceous earth, bentonite, activated carbon particles, nano-zinc oxide, nano-calcium oxide, and nano-alumina to a grinder for grinding, and then pass through a 100-mesh sieve to obtain a mixture A;
[0024] B. Add modified potassium hydroxide to the mixture A, mix and add to the stirring tank for full stirring, the stirring speed is 800 rpm, and the time is 40min, to obtain the mixture B; ...