Embodiment 1
[0034] Embodiment 1: a kind of environment-friendly size, including raw corn starch and size auxiliary agent, wherein size auxiliary agent is made up of starch viscosity reducer, plasticizer, wetting and penetrating agent, softening and smoothing agent and defoamer,
[0035] The slurry additive is made from the following raw materials by mass percentage:
[0036]
[0037]The steps for preparing the slurry additive are as follows: install the condenser tube, the stirrer and the three-necked flask; Put the starch viscosity reducer, wetting and penetrating agent, and smoothing agent into a three-necked flask, set the temperature at 55°C, stir for 30 minutes, and pour it into a beaker; place the beaker in a high-speed emulsifier, set the speed at 5000r / min, and the emulsification time After 30 minutes, add a specified amount of plasticizer and defoamer compound to emulsify at a low speed for 20 minutes to obtain a translucent white emulsion, take it out, adjust the pH value to ...
Embodiment 2
[0042] Embodiment 2: A new type of environment-friendly size aid is composed of two parts, including corn starch and size aid, wherein the size aid is composed of starch viscosity reducer, plasticizer, wetting and penetrating agent, softening and smoothing agent and defoamer composition.
[0043] The slurry additive is made from the following raw materials by mass percentage
[0044]
[0045] The steps for preparing the slurry additive are as follows: install the condenser tube, the stirrer and the three-necked flask; Put the starch viscosity reducer, wetting and penetrating agent, and smoothing agent into a three-necked flask, set the temperature at 60°C, stir for 30 minutes, and pour it into a beaker; place the beaker in a high-speed emulsifier, set the speed at 5000r / min, and the emulsification time After 30 minutes, add a specified amount of plasticizer and defoamer compound to emulsify at a low speed for 20 minutes to obtain a translucent white emulsion. Take it out ...