A polyethylene fiber and production process technology, which is applied in the field of chemical fiber production, can solve the problems of slow water dispersion, poor moisture permeability, and decreased air permeability, and achieve high production efficiency, improved modification effect, and weight reduction.

Inactive Publication Date: 2019-02-22
广东彩艳股份有限公司
View PDF1 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] Natural fibers take cotton as an example. It has good hygroscopicity and is comfortable to wear. However, when the human body sweats a little, the cotton fiber will swell due to moisture absorption, and its air permeability will decrease and it will stick to the skin.
At the same time, the water dispersion speed is also slow, causing a cold and wet feeling to the human body; synthetic fibers such as polyester have low water absorption and poor moisture permeability. Due to the accumulation of static electricity, it is easy to cause troubles when wearing, especially It is easy to feel stuffy during activities; special-shaped polyester fibers have the functions of perspiration and moisture conduction, but the surface of this type of material is rough and the comfort is poor

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Production technology of coated modified polyethylene fibers
  • Production technology of coated modified polyethylene fibers
  • Production technology of coated modified polyethylene fibers

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0022] A production process for coating modified polyethylene fibers, comprising the following steps:

[0023] (1) polyethylene and polyethylene terephthalate are respectively melted and extruded by a screw to obtain molten polyethylene material and molten polyethylene terephthalate material;

[0024] (2) In a mass ratio of 55:45, the molten polyethylene material is coated on the surface of the molten polyethylene terephthalate material to obtain polyester-modified polyethylene; The ethylene glycol phthalate material is realized by a bath tank loaded with molten polyethylene material with a flow rate of 0.5g / min per hole;

[0025] (3) cooling the polyester-modified polyethylene, adding an oil agent to the surface of the polyethylene to obtain a semi-finished product coated with modified polyethylene fibers;

[0026] (4) The coated modified polyethylene fiber semi-finished product is stretched in hot water at a temperature of 70°C, steam stretched at a temperature of 125°C, st...

Embodiment 2

[0028] A production process for coating modified polyethylene fibers, comprising the following steps:

[0029] (1) Polyethylene and polytrimethylene terephthalate are melted and extruded by screw respectively to obtain molten polyethylene material and molten polytrimethylene terephthalate material;

[0030] (2) In terms of a mass ratio of 50:50, the molten polyethylene material is coated on the surface of the molten polytrimethylene terephthalate material to obtain polyester-modified polyethylene; The propylene glycol formate material is realized by a bath tank loaded with molten polyethylene material with a flow rate of 0.45g / min per hole;

[0031] (3) cooling the polyester-modified polyethylene, adding an oil agent to the surface of the polyethylene to obtain a semi-finished product coated with modified polyethylene fibers;

[0032] (4) The coated modified polyethylene fiber semi-finished product is stretched in hot water at a temperature of 80°C, steam stretched at a tempe...

Embodiment 3

[0034] A production process for coating modified polyethylene fibers, comprising the following steps:

[0035] (1) polyethylene and polybutylene terephthalate are respectively melted and extruded by a screw to obtain molten polyethylene material and molten polybutylene terephthalate material;

[0036] (2) In a mass ratio of 45:55, the molten polyethylene material is coated on the surface of the molten polybutylene terephthalate material to obtain polyester-modified polyethylene; Butylene phthalate material is realized by the bath tank that is loaded with molten polyethylene material with flow rate as the trickle of 0.4g / min hole;

[0037] (3) cooling the polyester-modified polyethylene, adding an oil agent to the surface of the polyethylene to obtain a semi-finished product coated with modified polyethylene fibers;

[0038] (4) The coated modified polyethylene fiber semi-finished product is stretched in hot water at a temperature of 90°C, steam stretched at a temperature of 1...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
densityaaaaaaaaaa
densityaaaaaaaaaa
elongation at breakaaaaaaaaaa
Login to view more

Abstract

The invention relates to the technical field of chemical fiber production and in particular relates to a production technology of coated modified polyethylene fibers. The production technology comprises the following steps: (1) melting and extruding polyethylene and polyester respectively through a screw rod, so as to obtain a melted polyethylene material and a melted polyester material; (2) coating the surface of the melted polyester material with the melted polyethylene material according to the mass ratio of (45 to 70) to (30 to 55), so as to obtain polyester modified polyethylene, whereinthe step of coating is realized by enabling the melted polyester material to pass through a bath groove containing the melted polyethylene material in a fine flow manner; (3) cooling the polyester modified polyethylene; then adding an oil agent on the surface of the polyethylene to obtain a coated modified polyethylene fiber semi-finished product; and (4) carrying out stretching, curling and thermal setting on the coated modified polyethylene fiber semi-finished product to obtain the coated modified polyethylene fibers. The coated modified polyethylene fibers obtained by the production technology have the advantages of high strength, uneasiness of being deformed after stretching, high cohesive force, uneasiness of generating static electricity and good comprehensive performance, and are applicable to textile fabrics.

Description

technical field [0001] The invention relates to the technical field of chemical fiber production, in particular to a production process for coating modified polyethylene fibers. Background technique [0002] In recent years, with people's yearning and pursuit of a better life, the requirements for the comfort, health, safety and environmental protection of clothing fabrics are getting higher and higher. As people spend more time outdoors, the trend of mutual penetration and integration of casual wear and sportswear is increasingly favored by consumers. The fabrics of this type of clothing not only require good comfort, but also need to not stick to the skin and produce a cold and wet feeling once sweating occurs during activities. The performance of the fiber directly affects the function of the fabric, therefore, the fiber used needs to have comfortable and moisture-wicking properties. [0003] Natural fibers take cotton as an example. It has good hygroscopicity and is co...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): D06M15/507D06M101/20
CPCD06M15/507D06M2101/20D06M2200/50
Inventor 陈维壮李宇恒梁立峰黄华敬
Owner 广东彩艳股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products