Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

A kind of magnesium slag granulation method

A magnesium slag and granulation technology, which is applied in the field of resource utilization of solid waste, can solve the problems of increasing the cost of resource utilization of magnesium slag and difficulty in industrial application, and achieves the goals of promoting utilization and recycling, improving mineralization, and low cost Effect

Active Publication Date: 2021-03-23
NANJING KISEN INT ENG
View PDF6 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] The patent document with the application number CN201110027740.0 adopts the method of adding a small amount of boric acid into the magnesium slag, and then roasting the powdered γ-C 2 S converted to β-C 2 S, to obtain bulk waste slag, which improves the volume stability of magnesium slag by chemical methods. This method is based on the magnesium slag produced after the Pidgeon method of magnesium smelting, and needs to be calcined after the addition of modifiers, which greatly increases The cost of resource utilization of magnesium slag is reduced; the patent document whose application number is CN200910020830.X adopts the method of adding 3-15% aluminum-containing raw material additives in the raw material for producing magnesium metal, and then quenches the magnesium slag after calcining to obtain Bulk magnesium slag, but in my country's Pidgeon process magnesium smelting plant, it is still unable to achieve full automation. The current slag extraction still uses mechanical equipment as the main method, and artificial methods as the auxiliary method. The rapid cooling method is difficult to achieve large-scale industrial application.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] A method for granulating magnesium slag, comprising the steps of:

[0019] Step 1: Mix waste glass and borax at a mass ratio of 20:1, then crush and ball-mill the mixture to obtain a magnesium slag optimizer with a fineness of 45 μm and a sieve residue of less than 15%;

[0020] The second step: use calcined dolomite, ferrosilicon reducing agent and mineralizer as raw materials for producing magnesium metal, add magnesium slag optimization agent to the crushed raw materials for producing magnesium metal and mix them uniformly to form a mixture; wherein, in the mixture The mass content of each substance is respectively: 75% of calcined dolomite, 15% of ferrosilicon reducing agent, 0.3% of fluorite (mineralizing agent), and the balance is magnesium slag optimizing agent.

[0021] The third step: put the mixed material (pressed into balls) in the reduction tank, and carry out magnesium smelting according to the Pidgeon method. During the magnesium smelting process, metal m...

Embodiment 2

[0024] A method for granulating magnesium slag, comprising the steps of:

[0025] Step 1: Mix waste glass and borax at a mass ratio of 30:1, then crush and ball-mill the mixture to obtain a magnesium slag optimizer with a fineness of 45 μm and a sieve residue of less than 15%;

[0026] The second step: use calcined dolomite, ferrosilicon reducing agent and mineralizer as raw materials for producing magnesium metal, add magnesium slag optimization agent to the crushed raw materials for producing magnesium metal and mix them uniformly to form a mixture; wherein, in the mixture The mass content of each substance is respectively: 75% of calcined dolomite, 15% of ferrosilicon reducing agent, 0.3% of fluorite (mineralizing agent), and the balance is magnesium slag optimizing agent.

[0027] The third step: put the mixed material (pressed into balls) in the reduction tank, and carry out magnesium smelting according to the Pidgeon method. During the magnesium smelting process, metal m...

Embodiment 3

[0030] A method for granulating magnesium slag, comprising the steps of:

[0031] Step 1: Mix waste glass and borax at a mass ratio of 40:1, then crush and ball-mill the mixture to obtain a magnesium slag optimizer with a fineness of 45 μm and a sieve residue of less than 15%;

[0032] The second step: use calcined dolomite, ferrosilicon reducing agent and mineralizer as raw materials for producing magnesium metal, add magnesium slag optimization agent to the crushed raw materials for producing magnesium metal and mix them uniformly to form a mixture; wherein, in the mixture The mass content of each substance is respectively: calcined dolomite 80%, ferrosilicon reducing agent 15.5%, fluorite (mineralizing agent) 0.3%, and the balance is magnesium slag optimizing agent.

[0033] The third step: put the mixed material (pressed into balls) in the reduction tank, and carry out magnesium smelting according to the Pidgeon method. During the magnesium smelting process, metal magnesiu...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention provides a magnesium slag granulation method, which comprises the following steps of 1, mixing waste and abandoned glass and borax according to a mass ratio of (20 to 50):1; then, performing crushing and ball milling on the mixed material to obtain a magnesium slag optimizing agent; 2, using calcined dolomite, a silicon iron reducing agent, a mineralizer as metallic magnesium production raw materials; adding a certain amount of magnesium slag optimizing agent into the metallic magnesium production raw materials; performing uniform mixing to form a mixed material; 3, putting the mixed material into a reduction tank; smelting magnesium according to a Pidgeon process; in the magnesium smelting process, separating out metallic magnesium in a steam form; the waste slag is coated with a liquid phase formed by the magnesium slag optimizing agent; a hard shell body is formed after natural cooling; granulous magnesium slag is finally obtained. The method provided by the inventionhas the advantages that the process is simple; the cost is low; the granulation and agglomeration of the magnesium slag are completed in one step in the metallic magnesium smelting process; meanwhile,the consumption of the mineralizer can be reduced.

Description

technical field [0001] The invention relates to the technical field of resource utilization of solid waste, in particular to a magnesium slag granulation method. Background technique [0002] my country is the world's largest producer of magnesium metal. In recent years, my country's magnesium output has reached more than 70% of the world's total. my country's Ningxia, Shaanxi, Shanxi and other provinces are the main magnesium metal producers, and most of the current The production of metal magnesium all uses the Pidgeon method, and the Pidgeon method for smelting magnesium is currently the most mature method. The raw materials used in the Pidgeon method for smelting magnesium are dolomite and ferrosilicon as a reducing agent, and the calcined dolomite is mixed with ferrosilicon, and then mixed with mineralizer (CaF 2 ) according to the proportion of grinding, mixing and pressing into balls, and then put the balls into the reduction tank, after high temperature and high vacu...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C04B5/00C04B5/06
CPCC04B5/00C04B5/06
Inventor 武艳文钟根康宇王飞
Owner NANJING KISEN INT ENG
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products