Curing agent for rapidly curing river silt with high water content, and preparation method of curing agent
A technology for rapid solidification of river silt, applied in the field of curing agents, can solve problems such as insufficient treatment of high water content silt, and achieve the effects of improving precipitation efficiency, reducing precipitation costs, and improving efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] The silt is taken from a certain river in Jiangsu, with a moisture content of 240%-250%. The curing agent components are 50 parts of steel slag powder, 10 parts of cement, 20 parts of lime, 8 parts of gypsum, 4 parts of rubber powder, 3 parts of polyglycerin, 5 parts of polymethacrylate hydrogen, 2 parts of polyethylene wax-2000, aluminum acid Sodium 5 parts, dioctyl phthalate 4 parts. After the sludge is solidified, it can change from a high water content fluid plastic shape to a soft plastic shape within 30 minutes, and its liquidity index IL is 0.75. The unconfined compressive strength of the solidified soil after 7 days and 28 days of standard curing are respectively 183kPa and 294kPa, the mechanical properties of the silt are well improved.
Embodiment 2
[0028] The silt is taken from a certain river in Jiangsu, with a moisture content of 240%-250%. The curing agent consists of 45 parts of steel slag powder, 8 parts of cement, 20 parts of lime, 8 parts of gypsum, 4 parts of rubber powder, 2 parts of polyglycerin, 3 parts of polymethacrylate hydrogen, 1 part of polyethylene wax-2000, and 3 parts of sodium aluminate , 2 parts of dioctyl phthalate. After the sludge is solidified, it can change from a high water content fluid plastic state to a soft plastic state within 30 minutes. The measured liquidity index IL is 0.95, and the unconfined compressive strength of the solidified soil is 105kPa after standard curing for 7d and 28d. and 201kPa, the mechanical properties of the sludge are well improved.
Embodiment 3
[0030] The silt is taken from a certain river in Jiangsu, with a moisture content of 240%-250%. The curing agent consists of 50 parts of steel slag powder, 10 parts of cement, 15 parts of lime, 8 parts of gypsum, 3 parts of rubber powder, 3 parts of polyglycerin, 3 parts of polymethacrylate hydrogen, 1 part of polyethylene wax-2000, and 5 parts of sodium aluminate , 2 parts of dioctyl phthalate. After the sludge is solidified, it can change from high water content flow plastic to soft plastic within 30 minutes. The measured liquidity index IL is 0.95, and the unconfined compressive strength of the solidified soil after standard curing for 7d and 28d is 132kPa respectively and 225kPa, the mechanical properties of the sludge are well improved.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com