Disperse dye polyster dyeing method using siloxane as medium
A technology of disperse dyes and dyeing methods, applied in the field of textile ecological dyeing and finishing, can solve other ecological problems, high equipment dependence, difficult waste water treatment and other problems, and achieve the effects of less equipment dependence, easy media recovery, and less additives.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Take 30g of disperse red dye and 200g of siloxane medium to prepare a dye solution for later use. Get 6kg of polyester fiber and put it into siloxane medium, liquor ratio 1:4.5, add dyeing solution and 500g ethyl acetate, keep 7 o C / min heating up to 80 o C, keep 2 o C / min heating up to 140 o C, keep warm for 60min, quickly cool down and remove the liquid, then add siloxane medium, with 7 o C / min heating up 80 o C to keep warm for 10 minutes, wash twice in total, and finally deliquify and dry to obtain the finished dyed product.
[0024]
Embodiment 2
[0026] Take 10g of disperse orange dye and 200g of siloxane medium to prepare a dye solution for later use. Take 1.5kg of polyester fiber and put it into siloxane medium, bath ratio 1:5, add dye solution and 50% ethanol, keep 5 o C / min heating up to 80 o C, keep 3 o C / min heating up to 140 o C, keep warm for 50min, quickly cool down and remove the liquid, then add siloxane medium, with 8 o C / min heating up to 90 o C to keep warm for 10 minutes, wash twice in total, and finally deliquify and dry to obtain the finished dyed product.
[0027]
Embodiment 3
[0029] Take 0.1g of disperse blue dye and 1g of siloxane medium to prepare a dye solution for later use. Take 10g of polyester fiber and put it into siloxane medium, the bath ratio is 1:10, add dyeing solution, keep 7 o C / min heating up to 80 o C insulation for 30min, the insulation process is divided into four equal parts, the first three parts are three times to add dye solution, the last part is to add 1g acetic acid, keep 2 o C / min heating up to 140 o C, keep warm for 60min, quickly cool down and remove the liquid, then add siloxane medium, with 7 o C / min heating up 80 o C to keep warm for 10 minutes, wash twice in total, and finally deliquify and dry to obtain the finished dyed product.
[0030]
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com