High-stability leather fat-liquoring agent and preparation method
A kind of leather fatliquor, high stability technology, applied in leather impregnation, small raw hide/large raw hide/leather/fur treatment, small raw hide/large raw hide/leather hide/fur chemical treatment, etc., can solve the effect of fatliquoring treatment To be improved, storage stability and poor acid and alkali metal ion stability, etc., to achieve good emulsification effect, good storage stability, good natural gloss effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Embodiment 1: a kind of high stability leather fatliquoring agent, it is made up of the raw material composition of following parts by weight: 55 parts of modified ox hoof oils, 20 parts of beeswax liquids, 15 parts of triethylene glycol, isodecyl 12 parts of triol myristate, 8 parts of oleyl alcohol polyoxyethylene ether, 8 parts of coconut acid diethanolamide, 1.5 parts of petrolatum, and 70 parts of water.
[0020] Further, the preparation method of the modified cow's hoof oil is: stirring and reacting the cow's hoof oil with 15% diethanolamine of the cow's hoof oil and 1.2% of the cow's hoof oil with sodium methoxide at 60°C 4h to obtain the primary modified ox hoof oil; then lower the temperature to 45°C, add phosphorus pentoxide powder with a mass percentage of 45% of the primary modified ox hoof oil, after the addition is completed, raise the temperature to 75°C and keep it warm for 3 hours, and neutralize to pH 6 to 7 to obtain modified ox hoof oil; said phospho...
Embodiment 2
[0027] Embodiment 2: a kind of high stability leather fatliquoring agent, it is made up of the raw material composition of following parts by weight: 50 parts of modified ox hoof oils, 15 parts of beeswax liquids, 10 parts of triethylene glycol, isodecyl 8 parts of triol myristate, 5 parts of oleyl alcohol polyoxyethylene ether, 5 parts of coconut acid diethanolamide, 1 part of petrolatum, 65 parts of water.
[0028] Further, the preparation method of the modified cow's hoof oil is: stirring and reacting the cow's hoof oil with 10% by weight of cow's hoof oil of diethanolamine and 1% by weight of cow's hoof oil at 60°C 4h to obtain the primary modified ox hoof oil; then lower the temperature to 45°C, add phosphorus pentoxide powder with a mass percentage of 40% of the primary modified ox hoof oil, after the addition is completed, raise the temperature to 75°C and keep it warm for 3 hours, and neutralize to pH 6 to 7 to obtain modified ox hoof oil; said phosphorus pentoxide pow...
Embodiment 3
[0035] Embodiment 3: a kind of highly stable leather fatliquoring agent, it is made up of the raw material composition of following parts by weight: 60 parts of modified cow hoof oils, 25 parts of beeswax liquids, 15 parts of isotridecyl myristate, 10 parts of oleyl alcohol polyoxyethylene ether, 10 parts of coconut acid diethanolamide, 18 parts of triethylene glycol, 2 parts of vaseline, 75 parts of water.
[0036] Further, the preparation method of the modified cow's hoof oil is: stirring and reacting the cow's hoof oil with diethanolamine whose mass percentage is 20% of the cow's hoof oil and 1.5% by mass of the cow's hoof oil 4h to obtain primary modified ox hoof oil; then lower the temperature to 45°C, add phosphorus pentoxide powder which is 50% of the mass percentage of primary modified ox hoof oil, after the addition is completed, heat up to 75°C and keep it warm for 3 hours, and neutralize to pH 6 to 7 to obtain modified ox hoof oil; said phosphorus pentoxide powder i...